The development of gallium nitride (GaN) power devices requires a reliable selective-area doping process, which is difficult to achieve because of ongoing challenges associated with the required etch-then-regrow process. The presence of silicon (Si) impurities of unclear physical origin at the GaN regrowth interface has proven to be a major bottleneck. This paper investigates the origin of Si contamination at the epitaxial GaN-on-GaN interface and demonstrates an approach that markedly reduces its impact on device performance. An optimized dry-etching approach combined with UV-ozone and chemical etching is shown to greatly reduce the Si concentration levels at the regrowth interface, and a significant improvement in a reverse leakage current in vertical GaN-based p–n diodes is achieved.
Identical GaN/AlN resonant tunneling diode structures were grown on free-standing bulk GaN at substrate temperatures of 760 °C, 810 °C, 860 °C, and 900 °C via plasma-assisted molecular beam epitaxy. Each sample displayed negative differential resistance (NDR) at room temperature. The figures-of-merit quantified were peak-to-valley current ratio (PVCR), yield of the device with room-temperature NDR, and peak current density (Jp). The figures-of-merit demonstrate an inverse relationship between PVCR/yield and Jp over this growth temperature series. X-ray diffraction and transmission electron microscopy were used to determine the growth rates, and layer thicknesses were used to explain the varying figures-of-merit. Due to the high yield of devices grown at 760 °C and 810 °C, the PVCR, peak voltage (Vp), and Jp were plotted vs device area, which demonstrated high uniformity and application tunability. Peak current densities of up to 1.01 MA/cm2 were observed for the sample grown at 900 °C.
The morphology of GaN-on-GaN vertical p-i-n diode devices after reverse-bias electrical stressing to breakdown has been investigated. All failed devices had irreversible structural damage, showing large surface craters that were ∼15–35 μm deep with lengthy surface cracks. Cross-sectional electron micrographs of failed devices showed substantial concentrations of threading dislocations around the cracks and near the crater surfaces. Progressive ion-milling across damaged devices revealed high densities of threading dislocations and the presence of voids beneath the surface cracks; these features were not observed in any unstressed devices. These results should serve as a useful reference for future reliability studies of vertical high-power GaN devices.
23 February 2021 in Journal of Electronic Materials