Hydrocarbon ionomers bear the potential to significantly lower the material cost and increase the efficiency of proton‐exchange membrane water electrolyzers (PEMWE). However, no fully hydrocarbon membrane electrode assembly (MEA) with a performance comparable to Nafion‐MEAs has been reported. PEMWE‐MEAs are presented comprising sPPS as membrane and electrode binder reaching 3.5 A cm−2 at 1.8 V and thus clearly outperforming state‐of‐the‐art Nafion‐MEAs (N115 as membrane, 1.5 A cm−2 at 1.8 V) due to a significantly lower high frequency resistance (57 ± 4 mΩ cm² vs 161 ± 7 mΩ cm²). Additionally, pure sPPS‐membranes show a three times lower gas crossover (1.1 mA cm−2) in a fully humidified surrogate test. Furthermore, more than 80 h of continuous operation is shown for sPPS‐MEAs in a preliminary durability test (constant current hold at 1 A cm−2 at 80 °C). These results rely on the unique transport properties of sulfonated poly(phenylene sulfone) (sPPS) that combines high proton conductivity with low gas crossover.
2 August 2018 in The Journal of Physical Chemistry Letters
Polymer electrolyte membrane (PEM) water electrolysis is a crucial technology for green hydrogen production. Hydrocarbon membranes are drawing a lot of attention due to potentially superior properties and the fact that common fluorinated polymers might face a potential ban. This study introduces a sulfonated poly(phenylene sulfone) (sPPS) membrane, reinforced with a poly(ether‐ether‐ketone) (PEEK) mesh. The reinforced membrane induces a drastic increase in dimensional stability, enabling direct anode casting—an essential step toward industrial manufacturing. It further exhibits a significant reduction in water uptake (115% vs 294% for pure sPPS) and a 40% lower H2‐crossover (0.18 mA cm−2) compared to the industry standard N115 (0.31 mA cm−2). Due to the lower thickness (74 vs 127 µm) and higher ion exchange capacity (IEC)(1.92 vs 0.89 mmol g−1), the PEEK‐sPPS membrane displays a substantially lower resistance (70 vs 159 mΩ cm2 for N115). This directly translates into a voltage reduction of ≈90 mV at 1 A cm−2 or ≈180 mV at 2 A cm−2, both typical operating current densities. Finally, PEEK‐sPPS exhibits the longest lifetime shown for hydrocarbon membranes with almost 650 h at 1 A cm−2 and a low degradation rate (80 µV h−1).
20 December 2022 in Journal of Materials Chemistry A
Several theories have been proposed to explain the co-existence of high conductivity and high salt concentration for water-in-salt electrolytes. Here, we fill the gap related to the structural, physical, and electrochemical properties of the LiTFSI–H 2 O binary system at high mol kg −1 .
The layered material Li 2 Sn 2 S 5 forms two hydrated solid phases under increasing humidity. Intercalated water hydrates the interlayer Li + ions and screens coulombic interactions, leading to a high in-plane mobility of both Li + and H 2 O.