This paper presents the results of a metallographic and tribological study of 86WC-10Co-4Cr coatings obtained by the HVOF method on the Termika-3 unit at varying spraying distances. The influence of spraying distance on the coating microstructure, phase composition, as well as mechanical and tribological properties, was studied. According to the results of the study, it was found that the optimum spraying distance for 86WC-10Co-4Cr coatings with improved wear resistance and hardness characteristics and low porosity is 300 mm.
Samples using powders of four different fractions, 15–20 μm, 20–30 μm, 30–40 μm and 40–45 μm, were fabricated to investigate the wear resistance, corrosion resistance and tribological properties of the 86WC-10Co-4Cr coating obtained using the HVOF method. The phase composition, microstructure and elemental distribution were analyzed using X-ray diffraction, scanning electron microscopy and energy dispersive spectroscopy techniques. The hardness was measured on a Vickers microhardness tester, the friction coefficient and wear rate were investigated using a tribometer, and the corrosion resistance was evaluated on an electrochemical corrosion station. The results showed that the cross-sectional microstructure of the coating is mainly represented by multifaceted WC crystals embedded in the Co-Cr matrix and the presence of lower tungsten carbides, particularly W2C. The 15–20 μm fraction particles were subjected to superheating, contributing to the decarburization process. The 20–30 µm and 30–40 µm sized particles prevented overheating and had a more homogeneous structure. The 40–45 µm powder fractions did not reach sufficient temperature for complete melting, resulting in the formation of pores in the coating layers. The phase composition of the coatings included WC, W2C and CoO phases. According to the results of the study, it was found that the optimal powder fraction for coating the 86WC-10Co-4Cr composition with improved characteristics is the fraction of the 20–30 µm sized particles.
The structural-phase composition and tribological and performance properties of coatings based on an 86WC-10Co-4Cr composition obtained by the HVOF method at varying (150 L/min, 170 L/min, 190 L/min) oxygen flow rates were studied. The results showed that the coefficient of friction of coatings in gear oil remained almost unchanged with the variation in oxygen flow rate. However, microhardness increased significantly with an increasing oxygen flow rate, reaching a maximum at 190 L/min. An increasing oxygen flow rate was also accompanied by an increase in roughness and coating thickness, with a decrease in porosity, particularly notable at 190 L/min. Adhesion strength reached the maximum values for the A2 and A3 coatings under high loads. The phase composition of the coatings included WC, W2C and CoO phases irrespective of the oxygen flow rate, and their microstructure was characterized by a more homogeneous and dense structure. Thus, this study confirmed that the optimal oxygen flow rate for achieving an improved performance and tribological characteristics of 86WC-10Co-4Cr coatings is 190 L/min.
In this work, two configurations of Ti/HAp functionally graded coatings were fabricated on Ti–6Al–4V alloy substrates using detonation spraying. The coatings differed in the number and sequence of Ti and hydroxyapatite (HAp) deposition cycles, resulting in distinct gradient architectures: Configuration 1 incorporated a sharper transition from the Ti-rich base to the HAp-rich surface, whereas Configuration 2 featured a smoother and more gradual compositional gradient. The microstructure and elemental distribution were examined by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). Both configurations exhibited well-defined gradient layering, with titanium concentrated near the coating–substrate interface and an increased Ca and P content toward the upper bioceramic region. Raman spectroscopy confirmed the preservation of hydroxyapatite as the main phase, showing a characteristic 961 cm−1 band. Adhesion strength measured according to ASTM C633-13 was 45.78 ± 4.4 MPa for Configuration 1 and 52.32 ± 6.7 MPa for Configuration 2, both significantly exceeding the minimum required 15 MPa. The findings demonstrate that detonation-sprayed Ti/HAp gradient coatings provide strong adhesion and stable bioceramic surfaces, making them promising for metal implant applications.
This paper discusses the process of high-velocity oxygen fuel (HVOF) spraying with modeling of the gas flow parameters and behavior of WC-Co-Cr powder particles of different fractions (up to 20 µm, 21–35 μm and 36–45 μm). It was found that the temperature of the gas stream reaches a maximum of about 2700 °C, after which it gradually decreases, and the pressure in the combustion chamber (before the exit of gases through the nozzle) reaches maximum values, exceeding 400,000 Pa, and the pressure at the exit of the nozzle stabilizes at about 100,000 Pa, which corresponds to the standard atmospheric pressure. The gas velocity increases to 1300–1400 m/s and then decreases to 400 m/s at a distance of about 150 mm. It was determined that powder particles of the 21–35 µm fraction provide more stable parameters of velocity and temperature. Small particles (up to 20 µm) lose velocity and temperature faster as they advance, which deteriorates the coating quality, which was also experimentally confirmed. All results obtained from the HVOF process modeling fully align with the data from experimental studies.
This work presents the results of research on the effect of a pulsed plasma treatment on the structure, phase composition, hardness, roughness, and elemental composition of Fe-TiB2-CrB2-based coatings. The Fe-TiB2-CrB2 coating was applied via the detonation method. Fe-TiB2-CrB2 powder mixtures were used for coating on AISI 1017 steel substrate with the coating surface being modified using a pulsed plasma treatment. The effects of the pulsed plasma treatment on the microstructure, phase composition, and mechanical properties of Fe-TiB2-CrB2 detonation coatings were investigated using an optical microscope, X-ray diffraction (XRD), scanning electron microscopy (SEM), a nanohardness tester, and a Leica 3D profilometer. The mechanical test results showed that the hardness of the Fe-TiB2-CrB2 coating increased from 8.22 Gpa to 15.6 GPa after the pulsed plasma treatment. The results of the tribological tests show that after the pulsed plasma treatment of Fe-TiB2-CrB2 coatings, a wear-resistant modified layer consisting of (Ti,Cr)B2 and alpha-Fe formed on its surface. It is determined that the surface modified coating layer has a low porosity compared to the coating base. In addition, it is determined that after the pulsed plasma treatment, a decrease in the average pore size is observed in the subsurface layer of the coating. The pulsed plasma treatment resulted in a decrease in the roughness parameter (Ra) from 12.2 μm to 6.6 μm, which is due to the melting of protruding particles.