Deep cryogenic aging (DCA) is a newly developed heat treatment technique for additive-manufactured metallic materials to reduce residual stress and improve their mechanical properties. In this study, AlSi10Mg alloy samples fabricated by selective laser melting were deep-cryogenic-treated at −160 °C and subsequently aged at 160 °C. Phase and microstructural analyses were conducted using X-ray diffraction, optical microscopy, scanning electron microscopy, and transmission electron microscopy, while the mechanical properties were evaluated through microhardness and tensile testing at room temperature. The results indicated that the DCA treatment did not have an effect on the morphology of the melt pools. However, it facilitated the formation of atomic clusters and nanoscale Si and β′ phases, as well as accelerating the coarsening of grains and the ripening of the eutectic Si phase. After DCA treatment, the mass fraction of the Si phase experienced an increase from 4.4% to 7.2%. Concurrently, the volume fraction of the precipitated secondary phases elevated to 5.1%. The microhardness was enhanced to 147 HV, and the ultimate tensile strength and yield strength achieved 495 MPa and 345 MPa, respectively, with an elongation of 7.5%. In comparison to the as-built specimen, the microhardness, ultimate tensile strength, and yield strength increased by 11.4%, 3.1%, and 19.0%, respectively. The improvement in mechanical properties is primarily attributed to the Orowan strengthening mechanism induced by the secondary phases.
13 August 2025 in Materials Science and Engineering: A
As a recently developed high-strength aluminium alloy used specifically for laser additive manufacturing, AlMgMnSc alloy possesses superior mechanical properties and excellent processability. Extreme high-speed laser deposition (EHLD) is a novel surface-modification technique, which is characterised by high depositing speed, rapid cooling, rate and minimal dilution rate. To offer a new method for surface repairing high-strength aluminium alloys, an AlMgMnSc alloy coating, containing two deposition layers, is prepared on a 6061 aluminium-alloy axle using the EHLD technique. Meanwhile, the microstructure, composition distribution, and microhardness variation of the fabricated coating are studied. The results reveal that the coating is dense and crack-free, which is well-bonded with the substrate. Additionally, layer 1 is mainly composed of large columnar and equiaxed grains, while layer 2 consists of a fully equiaxed grain structure with an average grain size of about 4.5 μm. Moreover, the microhardness of the coating (about 104~118 HV) is similar to the substrate (about 105 HV), proving the feasibility of repairing high-strength aluminium alloys using AlMgMnSc alloy powders through the EHLD technique.
Selective laser melted Al-Mn-Sc alloys have attracted considerable attention as heat-resistant aluminum alloys for additive manufacturing due to their outstanding room-temperature strength and good high-temperature microstructural stability. However, most reported Al-Mn-Sc alloys rely on Mg addition for solid-solution strengthening, which, due to the high diffusivity of Mg, results in relatively low high-temperature strength and thus limits their application at elevated temperatures. Consequently, a Mg-free, Nd-modified AlMn5Sc0.7 alloy was designed and the effects of aging treatment on microhardness, microstructure, and tensile properties were investigated. The results demonstrate that the optimal aging condition for the alloy is 325 °C for 9 h, which represents a peak microhardness of 173 Hv0.05, representing a 44% improvement over the as-built condition. Aging treatment not only increases the volume fraction of primary phases but also induces the precipitation of secondary Al3Sc phases, characterized by a volume fraction of approximately 1.3% and an average size of about 1.5 nm. After heat treatment, the room-temperature ultimate tensile strength and yield strength of the alloy improve from 350 MPa and 310 MPa to 500 MPa and 470 MPa, respectively, primarily due to the modulus strengthening effect of the secondary Al3Sc. Meanwhile, at 250 °C and a strain rate of 8.3×10-5 s-1, the heat-treated alloy retains a high yield strength of 244 MPa. This excellent high-temperature strength arises mainly from the superior thermal stability of the primary and secondary phases, coupled with their effective pinning of grain boundaries and dislocations.