Deep cryogenic aging (DCA) is a newly developed heat treatment technique for additive-manufactured metallic materials to reduce residual stress and improve their mechanical properties. In this study, AlSi10Mg alloy samples fabricated by selective laser melting were deep-cryogenic-treated at −160 °C and subsequently aged at 160 °C. Phase and microstructural analyses were conducted using X-ray diffraction, optical microscopy, scanning electron microscopy, and transmission electron microscopy, while the mechanical properties were evaluated through microhardness and tensile testing at room temperature. The results indicated that the DCA treatment did not have an effect on the morphology of the melt pools. However, it facilitated the formation of atomic clusters and nanoscale Si and β′ phases, as well as accelerating the coarsening of grains and the ripening of the eutectic Si phase. After DCA treatment, the mass fraction of the Si phase experienced an increase from 4.4% to 7.2%. Concurrently, the volume fraction of the precipitated secondary phases elevated to 5.1%. The microhardness was enhanced to 147 HV, and the ultimate tensile strength and yield strength achieved 495 MPa and 345 MPa, respectively, with an elongation of 7.5%. In comparison to the as-built specimen, the microhardness, ultimate tensile strength, and yield strength increased by 11.4%, 3.1%, and 19.0%, respectively. The improvement in mechanical properties is primarily attributed to the Orowan strengthening mechanism induced by the secondary phases.

18 April 2019 in Coatings
Verified
Journal Article
Open access
PDF file
XLXiaodong Li
Xiaodong Li
SLShasha Liu
Shasha Liu
JWJiawei Wang
Jiawei Wang
MYMengxiao Yu
Mengxiao Yu
HTHaibo Tang
Haibo Tang
In order to improve the wear resistance of TC11 titanium alloy, a mixture of ZrN (10 wt.%, 20 wt.%, 30 wt.%, and 40 wt.%) and TC11 alloy powders are laser cladded on a forged TC11 substrate. The microstructure and wear property of coatings are systematically analyzed. The results show that the microstructure of sample with 10 wt.% ZrN addition has a very fine α + β two-phase microstructure, powders of ZrN are fully melted with no new phase appearance. By increasing the amount of ZrN to 20 wt.%, new phases of TiN0.3 precipitate with the dendritic morphology in the coating. A further increase in ZrN to 30 wt.% and 40 wt.% do not significantly change the microstructure of the cladded layer but increase the microhardness significantly, phases of TiN form with further enhancement of coating hardness. At the bottom of the cladded layer, the morphology of TiN0.3 and TiN precipitations changes into a spherical shape with small size. However, the wear performance of the coatings gradually reduces due to the increase of brittleness, and the superior wear properties of the coating are achieved when sample consisted of 20 wt.% ZrN.

30 April 2024 in Metals
Verified
Journal Article
Open access
PDF file
YYYancheng Yang
Yancheng Yang
YHYi Hu
Yi Hu
HCHongyan Chen
Hongyan Chen
YLYu Li
Yu Li
JWJiawei Wang
Jiawei Wang
DLDong Liu
Dong Liu
The microstructure characteristics of TiAl alloy prepared by laser-directed energy deposition (L-DED) are coarse columnar grains parallel to the building direction, which results in serious mechanical properties and anisotropy and limits its application. In the present study, TiB2 can be used as an effective grain refiner due to the extremely high Q value (growth inhibition factor; the larger the Q value of an alloying element, the stronger its grain refinement effect.) of B. With TiB2 addition, TiAl alloys prepared by laser-directed energy deposition with the microstructure of full equiaxed grains were obtained, and the grain size was significantly reduced by about 30% with 0.45 wt.% TiB2. This value has been further increased to 45% when adding 0.9 wt.% TiB2. Moreover, the γm phase was nearly eliminated and the width of (α2 + γ) lamellar was significantly decreased, which has positive effects on mechanical properties. Meanwhile, TiB2 precipitates uniformly distribute in the matrix, as a reinforced particle to increase the hardness and compressive strength of the alloys. The microhardness of the TiAl alloy increased with the increasing content of TiB2. The addition of TiB2 improved the room and high-temperature compressive properties of TiAl alloy while slightly increasing its ductility. These findings have important guiding significance for expanding the application of TiAl alloys.