A reliable local-fatigue assessment approach for rotary friction-welded components does not yet exist. The scope of this paper is to present test results for the fatigue behaviour of rotary friction-welded solid shafts made of structural steel S355J2G3 (1.0570) and an approach to fatigue assessment considering residual stress. In contrast to fusion-welded joints, components made by rotary friction welding usually contain compressive residual stress near the weld, which can significantly affect the fatigue strength. For this purpose, specimens were welded and characterised, including metallographic micrographs, hardness measurements, and residual stress measurements. The fatigue tests were performed with a constant amplitude loading in tension/compression or torsion with R = −1. All specimens were investigated without machining of the weld flash, either in the as-welded state or after a post-weld stress-relief heat treatment. In addition, the friction welding process and the residual stress formation were analysed using numerical simulation. The characterisation results are integrated into a fatigue assessment approach. Overall, the specimens perform comparatively well in the fatigue tests and the experimentally observed fatigue behaviour is well described using the proposed local approaches.
Application of cold gas spraying to the deposition of braze filler coatings has been investigated. Different light weight alloy substrates, i.e. aluminium AA1050, AA3005, AA5754, AA7022, magnesium AZ91 and titanium Ti–6Al–4V, were used. Filler coating materials depend on the substrate melting temperature. Therefore, for aluminium alloys Al–12Si zinc based fillers are used for AZ91 pure zinc and for Ti–6Al–4V different Cu–Ni blends are used. Cold gas spraying process parameters are varied with regard to process gas (nitrogen) temperature and pressure, powder feedrate and spray distance. Correlation of the process characteristics to economical aspects is given. The viability of the filler coatings produced is illustrated by different optimised brazing/soldering processes. In the case of aluminium braze joints a full metallographical investigation was carried out by optical and scanning electron microscopy as well as EDX analyses. The results obtained are compared with those of conventional filler material additions.
Rotary friction welding is a fast and efficient joining process with the possibility to join materials that are not weldable by conventional GMAW-processes. If done properly, the welds have a static and fatigue strength higher than the base material. However, in literature, there exists only sparse information on the design and assessment of these joints in terms of fatigue. The fatigue strength of two material combinations, S355-S355 and S355-1.4301, is investigated based on two specimen conditions, (1) with flash and (2) with flash mechanically removed. In the majority of tests, failure occurred outside the weld zone, in the base material. The derived endurable nominal stresses are compared to the design S-N curve of conventionally welded specimens and show a more than 50% higher fatigue strength.