In this study, based on a novel support vector machine optimization method, a wide processing window for manufacturing defect-free S25C carbon steel by electron beam powder bed fusion (EB-PBF) was identified. Samples with same energy densities exhibited similar microstructures and mechanical properties. One sample showed an optimum strength and elongation combination of 459.3 MPa and 57.6 pct. The pearlite region with irregular cementite particles was the first to crack during deformation, and the cracks gradually expanded into the surrounding area. Ferrite, cellular structures, and pearlite with parallel and straight cementite particles could effectively modulate the deformation by slip and enhance the plasticity of the S25C parts. After quenching, the strength improved to an unprecedented value of 1722.5 MPa owing to the presence of martensite and dislocation entanglements, with an elongation of 16.8 pct. The strength decreased after further tempering, and the plasticity evidently increased, with an optimum strength and elongation combination of 722.7 MPa and 44.2 pct, respectively. The microstructure of tempered sample contained lath martensite, cementite particles, and sparse dislocation lines. These results demonstrate that the current method can serve as a powerful tool for effectively optimizing the high-dimensional parameters of the EB-PBF process to produce carbon steel with excellent mechanical properties.
Heat treatment is the critical step in achieving a refined microstructure and enhanced mechanical properties of TiAl-based alloys. This study investigated the influence of heat treatment temperature, cooling method, and heat treatment time on the microstructure and mechanical properties of an extruded powder metallurgy Ti-48Al alloy, and achieved the control of fully lamellar fine microstructures and the enhancement of performance through a simple heat treatment, rather than the traditional approach of homogenization followed by heat treatment. The results indicate that the heat treatment temperature determines the type of microstructure, while the cooling rate dictates the lamellar width. As the heat treatment temperature was increased from the two-phase region to the α single-phase region, the microstructure transitioned from duplex to near lamellar, and the alloy strength initially increased and then decreased, influenced by both the lamellar colony ratio and grain size. A rapid cooling rate (water quenching) induces a non-diffusive massive phase transformation, whereas a slow cooling rate (air cooling) gradually forms α2/γ lamellar colonies. Therefore, a suitable heat treatment regime for the powder metallurgy Ti-48Al alloy was determined to be 1340 °C/5 min/air cooling. The microstructure of the alloy was near lamellar, consisting of lamellar colonies approximately 50 μm and a small number of γ equiaxed grains of about 10 μm. Subsequently, the alloy exhibited a room temperature tensile strength of 784 MPa and a yield strength of 763 MPa, representing improvements of 17.0% and 38.7% over the extruded alloy, respectively. This research provides a reference for establishing a heat treatment process for powder metallurgy TiAl alloys.
25 April 2025 in Journal of Materials Engineering and Performance
Selective laser melting (SLM) produces elemental segregation and nonequilibrium secondary phases in GH4169 superalloys, but the effects of P and C variations on grain-boundary phase evolution and high-temperature tensile behavior remain unclear. Alloys with primarily varied P (0.034–0.058 wt.%) and C (0.009–0.066 wt.%) contents were fabricated and heat treated identically. Microstructures were characterized by scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM), and tensile properties were evaluated at 650 °C. The as-built alloys exhibited columnar grains, cellular substructures, cell-wall segregation, and Nb-rich Laves-phase particles. After heat treatment, cellular substructures largely disappeared, γ″ precipitates formed in the γ matrix, and fine Ti/Al-rich particles were tentatively attributed to γ′; δ phase, residual Laves phase, and MC-type carbides were present at grain boundaries. Increasing P reduced the δ-phase area fraction from 2.20% to 1.38% and changed its distribution from continuous chains to semi-continuous and discrete arrangements. Increasing C raised the MC-type carbide area fraction from 0.34% to 1.48% while decreasing the δ-phase area fraction from 1.68% to 0.98%, accompanied by carbide coarsening. The 0.050P alloy exhibited the highest yield and ultimate tensile strengths, whereas the 0.009C alloy showed the best strength–ductility balance. These results reveal distinct P- and C-related changes in grain-boundary phase evolution and tensile behavior at 650 °C.