The influence of Cr addition on the microstructure and tensile properties of Fe-25Mn-10Al-1.2C lightweight steel was investigated. The characteristics of the microstructures and deformation behavior were carried out through X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), electron backscatter diffraction (EBSD), and room temperature tensile testing. Fe-20Mn-12Al-1.5C steel without Cr exhibited a fully austenitic single phase. With the addition of Cr, the volume fraction of ferrite continuously increased. When the content of Cr exceeded 5 wt%, the precipitation of Cr7C3 carbides was observed. In the steel with 5 wt% Cr, the quantity of κ carbides remarkably decreased, indicating that the addition of 5 wt% Cr significantly inhibited the nucleation of κ-carbides. As the Cr content increases from 0 wt% to 5 wt%, the austenite grain sizes were 8.8 μm and 2.5 μm, respectively, demonstrating that Cr alloying is an effective method of grain refinement. Tensile strength increased slightly while elongation decreased with increasing Cr content. As the Cr content exceeded 5 wt%, the yield strength increased but the elongation drastically decreased. The steel with 2.5 wt% Cr achieved a synergistic improvement in strength and ductility, exhibiting the best tensile performance.
The development of lightweight steels with high specific strength is critical for automotive applications and energy savings. This study aimed to develop a high-performance lightweight steel with high specific strength by designing an alloy composition and optimizing thermomechanical processing. A novel Fe-28.6Mn-10.2Al-1.1C-3.2Ni-3.9Cr (wt.%) steel was investigated, focusing on microstructural evolution, mechanical properties, and strengthening mechanisms. The steel was processed through hot-rolling, solution treatment, cold-rolling, and subsequent annealing. Microstructural characterization revealed a dual-phase matrix of austenite and ferrite (6.8 vol.%), with B2 precipitates distributed at the grain boundaries and within the austenite matrix, alongside nanoscale κ-carbides (<10 nm). Short-time annealing resulted in the finer austenite grains (~1.1 μm) and the higher volume fraction (5.0%) of intragranular B2 precipitates with a smaller size (~0.18 μm), while long-time annealing promoted the coarsening of austenite grains (~1.6 μm) and the growth of intergranular B2 particles (~0.9 μm). This steel achieved yield strengths of 1130~1218 MPa and tensile strengths of 1360~1397 MPa through multiple strengthening mechanisms, including solid solution strengthening, grain boundary strengthening, dislocation strengthening, and precipitation strengthening.
The effects of intercritical quenching on the microstructure evolution and mechanical performance of Cr–Ni–Mo–V steel with a banded structure are studied. It is found that the intercritical quenching temperature has a significant effect on the morphology, distribution, and relative amount of ferrite/martensite, as well as the carbide precipitates upon tempering treatment. It is indicated that owing to the initial banded structure of Cr-Ni-Mo-V steel, the ferrite formation in intercritical heat treatment also exhibits a banded distribution. With the increase in quenching temperature, the proportion of ferrite in the Cr-Ni-Mo-V steel decreases from 30 ± 3.2 vol.% to 18 ± 2.8 vol.%. Tempering treatment has no significant effect on the distribution characteristics of ferrite, but it promotes the recovery of martensite laths and the precipitation of carbides. The mechanical properties of Cr-Ni-Mo-V steel are determined by both the changes in ferrite content induced by intercritical quenching and the evolution of carbide types during tempering. Delamination cracks are observed on the fracture surface, which is attributed to the lamellar microstructure, improving the plasticity of Cr-Ni-Mo-V steel through stress dispersion and a multi-stage energy absorption mechanism.