Yunfei Du

Dr. Yunfei Du


Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 June 2024 in Metals
Verified
Journal Article
Open access
PDF file
RBRui Bai
Rui Bai
YDYunfei Du
Yunfei Du
XHXiuli He
Xiuli He
YZYaqin Zhang
Yaqin Zhang
The influence of Cr addition on the microstructure and tensile properties of Fe-25Mn-10Al-1.2C lightweight steel was investigated. The characteristics of the microstructures and deformation behavior were carried out through X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), electron backscatter diffraction (EBSD), and room temperature tensile testing. Fe-20Mn-12Al-1.5C steel without Cr exhibited a fully austenitic single phase. With the addition of Cr, the volume fraction of ferrite continuously increased. When the content of Cr exceeded 5 wt%, the precipitation of Cr7C3 carbides was observed. In the steel with 5 wt% Cr, the quantity of κ carbides remarkably decreased, indicating that the addition of 5 wt% Cr significantly inhibited the nucleation of κ-carbides. As the Cr content increases from 0 wt% to 5 wt%, the austenite grain sizes were 8.8 μm and 2.5 μm, respectively, demonstrating that Cr alloying is an effective method of grain refinement. Tensile strength increased slightly while elongation decreased with increasing Cr content. As the Cr content exceeded 5 wt%, the yield strength increased but the elongation drastically decreased. The steel with 2.5 wt% Cr achieved a synergistic improvement in strength and ductility, exhibiting the best tensile performance.

28 August 2025 in Materials
Verified
Journal Article
Open access
RBRui Bai
Rui Bai
YLYing Li
Ying Li
YDYunfei Du
Yunfei Du
YZYaqin Zhang
Yaqin Zhang
XHXiuli He
Xiuli He
HLHongyu Liang
Hongyu Liang
The development of lightweight steels with high specific strength is critical for automotive applications and energy savings. This study aimed to develop a high-performance lightweight steel with high specific strength by designing an alloy composition and optimizing thermomechanical processing. A novel Fe-28.6Mn-10.2Al-1.1C-3.2Ni-3.9Cr (wt.%) steel was investigated, focusing on microstructural evolution, mechanical properties, and strengthening mechanisms. The steel was processed through hot-rolling, solution treatment, cold-rolling, and subsequent annealing. Microstructural characterization revealed a dual-phase matrix of austenite and ferrite (6.8 vol.%), with B2 precipitates distributed at the grain boundaries and within the austenite matrix, alongside nanoscale κ-carbides (<10 nm). Short-time annealing resulted in the finer austenite grains (~1.1 μm) and the higher volume fraction (5.0%) of intragranular B2 precipitates with a smaller size (~0.18 μm), while long-time annealing promoted the coarsening of austenite grains (~1.6 μm) and the growth of intergranular B2 particles (~0.9 μm). This steel achieved yield strengths of 1130~1218 MPa and tensile strengths of 1360~1397 MPa through multiple strengthening mechanisms, including solid solution strengthening, grain boundary strengthening, dislocation strengthening, and precipitation strengthening.

27 August 2025 in Materials
Verified
Journal Article
Open access
YDYunfei Du
Yunfei Du
XZXiaosheng Zhou
Xiaosheng Zhou
RBRui Bai
Rui Bai
YZYaqin Zhang
Yaqin Zhang
The effects of intercritical quenching on the microstructure evolution and mechanical performance of Cr–Ni–Mo–V steel with a banded structure are studied. It is found that the intercritical quenching temperature has a significant effect on the morphology, distribution, and relative amount of ferrite/martensite, as well as the carbide precipitates upon tempering treatment. It is indicated that owing to the initial banded structure of Cr-Ni-Mo-V steel, the ferrite formation in intercritical heat treatment also exhibits a banded distribution. With the increase in quenching temperature, the proportion of ferrite in the Cr-Ni-Mo-V steel decreases from 30 ± 3.2 vol.% to 18 ± 2.8 vol.%. Tempering treatment has no significant effect on the distribution characteristics of ferrite, but it promotes the recovery of martensite laths and the precipitation of carbides. The mechanical properties of Cr-Ni-Mo-V steel are determined by both the changes in ferrite content induced by intercritical quenching and the evolution of carbide types during tempering. Delamination cracks are observed on the fracture surface, which is attributed to the lamellar microstructure, improving the plasticity of Cr-Ni-Mo-V steel through stress dispersion and a multi-stage energy absorption mechanism.

1 January 2024 in High Temperature Materials and Processes
Verified
Journal Article
Open access
PDF file
YDYunfei Du
Yunfei Du
RBRui Bai
Rui Bai
BWBo Wang
Bo Wang
LZLi Zhang
Li Zhang
GLGuodong Li
Guodong Li
On a Gleeble-3800 thermal simulator, the hot deformation behavior of Cr–Mo–Ni–V steel was studied, with the designed deformation temperature varying from 900 to 1,200°C and the strain rate in the range of 0.01–10 s −1 . It was observed that as the strain rate was increased and the hot working temperature was reduced, the flow stress of the experimental steel increased. The study also evaluated the safe parameters for deformation of the Cr–Mo–Ni–V steel in the hot working process, based on the established processing maps. It was found that the deformation temperature window varying from 1,050 to 1,150°C and the reasonable strain rate in the range of 0.01–1 s −1 are beneficial to the hot deformation of the steel. In this research, the effect of processing parameters of the hot working process on the microstructure evolution of the banded structure was also investigated. According to the research result, the banded structure in the steel remained visible under the conditions of a strain rate of 10 s −1 and the hot working temperature in the range of 900–1,200°C. However, it should be noted that the banded structure in the steel then gradually disappeared when the hot working temperature was increased to 1,200°C.