The effects of La and La+Sc addition on mechanical properties and thermal conductivity of Al-4.8Cu alloy were comprehensively studied. The as-cast samples were characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD) and first-principles methods. The results reveal that the grain morphology of Al-4.8Cu alloy changes from dendrite to fine equiaxed grain with La, La+Sc addition. The average grain size of Al-Cu-La (Al-4.8Cu-0.4La) and Al-Cu-La-Sc (Al-4.8Cu-0.4La-0.4Sc) decreased by 37.2% (70.36 μm) and 63.3% (119.64 μm) respectively compared with Al-Cu (Al-4.8Cu). Al-Cu-La has the highest elongation among the three which is 34.4% (2.65%) higher than Al-Cu. Al-Cu-La-Sc has the highest ultimate tensile strength and yield strength which are 55.1% (80.9 MPa) and 65.2% (62.1 MPa) higher than Al-Cu, respectively. The thermal conductivity of Al-Cu-La and Al-Cu-La-Sc is 10.0% (18.797 W·m−1·k−1) and 6.5% (12.178 W·m−1·k−1) higher than Al-Cu alloy respectively. Compared with Al-Cu, Al-Cu-La has less shrinkage and porosity, the presence of Al4La and AlCu3 contribute a lot to the decrease of specific heat capacity and the increase of plasticity and toughness. The porosity of Al-Cu-La-Sc does not significantly decrease compared with Al-Cu-La, the presence of Al3Sc and AlCuSc bring about the increase of specific heat capacity and brittleness.
1 November 2017 in Transactions of Nonferrous Metals Society of China
Effects of laser surface remelting (LSR) on microstructure and corrosion properties of as-cast Mg-12Dy-1.1Ni (wt.%) alloy were investigated. The as-cast alloy was mainly composed of α-Mg, lamellar Mg12DyNi phase with an 18R-long period stacking order (LPSO) structure and Mg24Dy5. After LSR treatment, fine and compact 18R-LPSO phase reprecipitated on dendrite boundaries as a continuous network. In addition, the volume fraction of the LPSO phase remarkably increased to 34.9% and the grain size of as-cast alloy was refined to ca. 4 μm. Electrochemical and immersion tests indicated that the LSR-treated alloy exhibited a lower weight loss rate (2.8 ± 0.2 mg/cm2/h) and corrosion current density (160.1 ± 20.7 μA/cm2, and of 37% reduction after LSR) than the as-cast alloy in 0.1 M NaCl solution. The improved corrosion resistance of the LSR alloy was mainly ascribed to the grain refinement and continuous distribution of 18R-LPSO phase on dendrite boundaries.
3 December 2023 in Journal of Materials Research and Technology