The effects of La and La+Sc addition on mechanical properties and thermal conductivity of Al-4.8Cu alloy were comprehensively studied. The as-cast samples were characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD) and first-principles methods. The results reveal that the grain morphology of Al-4.8Cu alloy changes from dendrite to fine equiaxed grain with La, La+Sc addition. The average grain size of Al-Cu-La (Al-4.8Cu-0.4La) and Al-Cu-La-Sc (Al-4.8Cu-0.4La-0.4Sc) decreased by 37.2% (70.36 μm) and 63.3% (119.64 μm) respectively compared with Al-Cu (Al-4.8Cu). Al-Cu-La has the highest elongation among the three which is 34.4% (2.65%) higher than Al-Cu. Al-Cu-La-Sc has the highest ultimate tensile strength and yield strength which are 55.1% (80.9 MPa) and 65.2% (62.1 MPa) higher than Al-Cu, respectively. The thermal conductivity of Al-Cu-La and Al-Cu-La-Sc is 10.0% (18.797 W·m−1·k−1) and 6.5% (12.178 W·m−1·k−1) higher than Al-Cu alloy respectively. Compared with Al-Cu, Al-Cu-La has less shrinkage and porosity, the presence of Al4La and AlCu3 contribute a lot to the decrease of specific heat capacity and the increase of plasticity and toughness. The porosity of Al-Cu-La-Sc does not significantly decrease compared with Al-Cu-La, the presence of Al3Sc and AlCuSc bring about the increase of specific heat capacity and brittleness.
The casting table with lubricating oil and wiper is applied simultaneously to produce super-high-strength 7055 aluminum alloy (Al7055) ingots, and 30 T Al7055 ingots with a diameter of 582 mm were cast successfully. In this study, the microstructure and macrosegregation of the ingots were investigated using an optical microscope (OM). The research results show that the hydrogen content in the liquid metal can be decreased from 0.198 mL/100 g Al to 0.103 mL/100 g Al when three rotors are used in the degassing tank. Compared with the conventional hot-top casting table, the surface quality can be improved by using the casting table with oil lubrication. The temperature gradient between the ingot center and edge can be decreased by using the wiper during the casting process from 320 °C to 150 °C, the cracking tendency caused by the ingot temperature gradient can be decreased, the segregation layer thickness is decreased by about 87%, and the ingot can be homogenized at a high temperature by using the heat of the feed itself.
An Al 6061/Mg AZ31B composite plate with good bonding and excellent comprehensive mechanical properties was prepared through solid-liquid cast-rolling bonding (SLCRB). The microstructure evolution and mechanical behavior of Al/Mg composite plates under different rolling passes were studied. The results showed that with the increase of rolling passes, the bonding layer of the composite plate was crushed, and the base material on both sides of the substrate gradually grew towards the broken part of the bonding layer. The microstructure on both sides of the substrate extended along the rolling direction and was dynamically recrystallized to a certain extent. In the Mg substrate, because the preheating temperature was higher than its recrystallization temperature, with the increase of rolling passes, the grains in Mg substrate were crystallized. When the rolling passes reached the fourth pass, complete recrystallization basically took place in the Mg substrate. With the change of the internal structure and bonding layer on both sides of the substrate, the mechanical properties of the composite plate can be improved gradually. The tensile strength increased from 136 MPa before rolling to 190 MPa at the fourth pass, and the shear strength increased from 74 MPa to 98 MPa, with growth rates of about 40% and 32%, respectively. The elongation of the composite plate decreased from 6.3% to 5.4%, a decrease of about 1%.