The primary objective of this paper is to investigate the influence of deformation degree on the microstructure and properties of a Ni-based superalloy. An upsetting experiment was conducted using a free-forging hammer to achieve a deformation degree ranging from 60% to 80%. The impact of the forging deformation degree on the hardness and high-temperature erosion performance was evaluated using the Rockwell hardness tester (HRC) and high-temperature erosion tester, respectively. The experimental results indicate that as the deformation degree increased, the hardness of the forged material progressively increased while the rate of high-temperature erosion gradually decreased. In order to comprehensively study the mechanism behind the variations in forging performance, optical microscopy (OM), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM) were employed. The findings reveal that as the deformation degree increased, the presence of small-angle grain boundaries and an increase in grain boundary area contributed to enhanced hardness in the alloy forgings. Furthermore, it was discovered that grain boundaries with twin orientation promoted dynamic recrystallization during deformation, specifically through a discontinuous dynamic recrystallization mechanism. Additionally, the precipitated γ′ phase in the alloy exhibited particle sizes ranging from 40 to 100 nm. This particle size range resulted in a higher critical shear stress value and a more pronounced strengthening effect on the alloy.
To investigate the effect of the primary γ′ phase on the high-temperature endurance performance of GH4720Li superalloy, samples with different volume fractions of the primary γ′ phase were prepared by adjusting the heat treatment process. The high-temperature endurance performance was tested, and the microstructure was examined. Results indicate that samples with a higher volume fraction of the γ′ phase exhibit a greater stress rupture life. Additionally, alloy samples with varying γ′ phase volume fractions show improved plasticity and toughness at 760 °C/530 MPa. Fracture morphology results reveal that high-volume-fraction primary γ′ phase samples primarily undergo transgranular fracture, whereas low-volume-fraction samples exhibit intergranular fracture due to grain boundary sliding. During high-temperature endurance, the secondary γ′ phase in the crystal is affected. Long-term aging refines the secondary γ′ phase, resulting in a more uniform distribution. Finally, the influence of the primary γ′ phase and the creep behavior of each material group on high-temperature endurance performance are discussed.
5 November 2025 in Journal of Materials Engineering and Performance