Although advancements in CAD/CAM technology allow for more personalized treatments, it is not clear how modifications in the CAD/CAM milling process could affect the restoration surface conditions and their mechanical behavior. The objective of this study was to evaluate the effect of different CAD/CAM milling protocols on the topography and fracture behavior of zirconia monolithic crowns (3Y-PSZ) subjected to a chewing simulation. Monolithic 3Y-PSZ premolar crowns were milled using three protocols (n = 13) (slow (S), normal (N), and fast (F)). Crowns were cemented on a dentin analog abutment and subjected to mechanical aging (200 N, 2 Hz, 1,500,000 cycles, 37 °C water). Surviving crowns were subjected to compressive load test and analyzed using fractography. Fracture load data were analyzed with two-parameter Weibull analysis. The surface topography of the crowns was examined with a stereomicroscope and a 3D non-contact profiler. All crowns survived the chewing simulation. Crowns milled using the F protocol had the greatest characteristic fracture load, while crowns produced with the S protocol showed high Weibull modulus. Groups N and S had a more uniform surface and detailed occlusal anatomy than group F. The CAD/CAM milling protocol affected the topography and mechanical behavior of 3Y-PSZ monolithic crowns.
This study aimed to investigate the failure behavior of 3 mol.% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) prosthetic crowns air-abraded with aluminum oxide (AO) particles of different sizes. Ninety ceramic premolar crowns were produced with 3Y-TZP frameworks veneered with porcelain. Crowns were randomly divided into three groups, according to the size of the air abrasion AO particles (n = 30): (GC) untreated (control); (G53) 53 µm; (G125) 125 µm. Air abrasion was performed with 0.25 mpa pressure, 10-mm distance, for 10 s. Crowns were adhesively cemented to dentin analog abutments. Specimens were loaded in compression to failure, in 37oC distilled water, using a universal testing machine (n = 30). Fractographic analysis was performed using a stereomicroscope and SEM. The roughness of the crown’s inner surface was evaluated using an optical profilometer (n = 10). Fracture load data were statistically analyzed with Weibull analysis and roughness data with Kruskal-Wallis (α = 0.05). GC had the lowest characteristic fracture load (L0), while G53 and G125 had higher and statistically similar L0 values. The Weibull modulus (m) was similar among groups. The failure modes observed were catastrophic failure and porcelain chipping. There were no differences between the roughness parameters for the experimental groups (p > 0.05). The size of the AO particles did not affect the fracture load and failure mode of 3Y-TZP crowns. Air abrasion with 53 µm and 125 µm particles resulted in a higher fracture load of ceramic crowns than the untreated group while maintaining their reliability and surface characteristics.
Repair in resin-based composite is a procedure that has shown good results, when properly indicated. In cases of fracture or stainning, the total removal of the restoration can cause unnecessary wear on the dental element. This study evaluated the aging effect on the bond strength of a universal adhesive containing silane, and/or application of silane separately for composite repairs. Resin composite blocks were thermocycled and divided according to adhesion protocol (n=10): silane(Sil), conventional adhesive(CA), universal adhesive(UA), Sil+CA(SilCA), and Sil+UA(SilUA). Layers of resin composite were added and blocks were sectioned and divided into 2 subgroups: 24h and 4 months of water storage. Microtensile bond strength test was performed and data were statistically analyzed (a = 0.05). After 4months of aging SilCA and SilUA showed a significant bond strength reduction, while for UA the bonding remained stable.
9 May 2026 in Journal of Esthetic and Restorative Dentistry
Objectives: Variables related to CAD/CAM processing can affect the final quality of all‐ceramic crowns. This study aims to evaluate the effect of the milling protocol on the adaptation, marginal and occlusal quality of monolithic zirconia crowns. Materials and Methods: Thirty‐nine monolithic zirconia crowns were produced using three CAD/CAM milling protocols ( n = 13): slow (S), normal (N), and fast (F). Adaptation (gap thickness) was evaluated using the replica technique, while marginal quality was assessed according to a severity scale. Occlusal quality was investigated qualitatively, using a stereomicroscope, and quantitatively, through an occlusal dimensional discrepancy analysis. Gap thickness and occlusal discrepancy data were analyzed with ANOVA and Tukey's test, and marginal quality with Kruskal–Wallis and Student–Newman–Keuls ( α = 0.05). Results: Gap thickness in the marginal, gingival‐axial angle and axial regions was similar among groups. In the axio‐occlusal angle and occlusal region, group N presented the smallest gap. For marginal quality, group F had higher scores in the severity scale than groups N and S for the mesial and buccal regions. Group F crowns showed less refined occlusal anatomy. Yet, when crowns produced with S and F protocols were compared with N, the total mean discrepancy was similar. Conclusion: The CAD/CAM milling protocol affected the adaptation, marginal, and occlusal quality of monolithic zirconia crowns.