The research shows that carbonation-cured concrete has several mechanical and durability properties that are better than those of moisture-cured concrete. However, many properties of carbonation-cured concrete have not yet been studied. In this research, carbonation-cured concrete was prepared by pre-curing, carbonation curing, and then moisture curing. The compressive strength, CO2 uptake, pH value, chloride ion permeability and abrasion resistance of the carbonation-cured concrete were investigated. Results showed that the compressive strength of carbonation-cured concrete was more than 10% higher than that of moisture-cured concrete at the same age; a steel bar is stable in carbonation-cured concrete; and carbonation-cured concrete exhibited better abrasion resistance and chloride ion permeability than that of moisture-cured concrete. The optimization of pore structure and improvement in the micro-hardness are the reasons for the improved chloride ion permeability and abrasion resistance of carbonation-cured concrete.
This paper presents a study on the carbonation reaction heat and products of tricalcium silicate (C3S) paste exposed to carbon dioxide (CO2) for rapid curing. Reaction heat was measured using a retrofitted micro-calorimeter. The highest heat flow of a C3S paste subject to carbonation curing was 200 times higher than that by hydration, and the cumulative heat released by carbonation was three times higher. The compressive strength of a C3S paste carbonated for 2 h and 24 h was 27.5 MPa and 62.9 MPa, respectively. The 24-h carbonation strength had exceeded the hydration strength at 28 days. The CO2 uptake of a C3S paste carbonated for 2 h and 24 h was 17% and 26%, respectively. The X-ray diffraction (XRD), transmission electron microscope coupled with energy dispersive spectrometer (TEM-EDS), and 29Si magic angle spinning–nuclear magnetic resonance (29Si MAS-NMR) results showed that the products of a carbonated C3S paste were amorphous silica (SiO2) and calcite crystal. There was no trace of calcium silicate hydrate (C–S–H) or other polymorphs of calcium carbonate (CaCO3) detected.
Influence of C12A7 (12CaO·7Al2O3) as a functional component on hydration properties of Ordinary Portland Cement is studied using isothermal microcalorimetric technique, X-ray diffraction analysis, and thermodynamic calculation. Meanwhile, hydrate assemblages are simulated by hydrothermal software. C2AH8 (2CaO·Al2O3·8H2O) is generated as a transition phase during the hydration of pure C12A7, while formation of CAH10 (CaO·Al2O3·10H2O) is uncertain. Heat-releasing behavior of Ordinary Portland Cement (OPC) could be noticeably affected by C12A7, especially for the duration of interaction at boundary stage reduces with C12A7 replacement. Correspondingly, all hydration kinetic parameters first increase and then diminish with C12A7 replacement. Simulation results manifest in the main hydration products of OPC being ettringite, C-S-H (Calcium-Silicate-Hydrate) gel, portlandite and brucite. Increasing C12A7 replacement accelerates the consumption rates of gypsum and calcite that are typically included in OPC, and thus the ettringite content is changed and carbonate phases will be produced. Therefore, the microstructure properties of hydrated products of OPC are affected and the compressive strength is influenced. These predications are in good agreement with experimental findings. C12A7 can be used as a functional component to adjust the consumption rate of suphates in OPC, and also components of carbonate phases can be modified in hydrate assemblage.
10 June 2022 in Journal of Wuhan University of Technology-Mater. Sci. Ed.