The research shows that carbonation-cured concrete has several mechanical and durability properties that are better than those of moisture-cured concrete. However, many properties of carbonation-cured concrete have not yet been studied. In this research, carbonation-cured concrete was prepared by pre-curing, carbonation curing, and then moisture curing. The compressive strength, CO2 uptake, pH value, chloride ion permeability and abrasion resistance of the carbonation-cured concrete were investigated. Results showed that the compressive strength of carbonation-cured concrete was more than 10% higher than that of moisture-cured concrete at the same age; a steel bar is stable in carbonation-cured concrete; and carbonation-cured concrete exhibited better abrasion resistance and chloride ion permeability than that of moisture-cured concrete. The optimization of pore structure and improvement in the micro-hardness are the reasons for the improved chloride ion permeability and abrasion resistance of carbonation-cured concrete.
In this paper, Ag-TiO2 photocatalysts with different Ag contents (1 mol%–5 mol%) were prepared and applied to cement mortar. The photocatalytic performance of Ag-TiO2 and photocatalytic cement mortar under UV light and simulated solar light was evaluated. The results showed that Ag loading on the surface of TiO2 could reduce its band gap width and increase its absorbance in the visible region, and 2% Ag-TiO2 had the highest photocatalytic activity under UV light, the degradation rate of methyl orange (MO) was 95.5% at 30 min, and the first-order reaction constant k was 0.0980 min−1, which was 61.7% higher than that of TiO2, and 5% Ag-TiO2 had the highest photocatalytic activity under solar light, the degradation rate of methylene blue (MB) was 69.8% at 40 min, and the first-order reaction constant k was 0.0294 min−1, which was 90.9% higher than that of TiO2. The photocatalytic mortar prepared by the spraying method has high photocatalytic performance, The MO degradation rate of sample S2 under UV light was 87.5% after 120 min, MB degradation rate of sample S5 under solar light was 75.4% after 120 min. The photocatalytic reaction conforms to the zero-order reaction kinetics, which was 1.5 times–3.3 times higher than that of the mixed samples and has no effect on the mechanical properties of mortar.
Using waste molecular sieves (MS) instead of sand as water-absorbing fine aggregates in cement-based materials can effectively deal with factory adsorption waste and reduce sand consumption. In this article, the industrial waste molecular sieve is recycled and incorporated into cement-based materials. The effect of the molecular sieve as a hydration internal curing agent on the performance of cement-based materials is studied. A series of experiments are designed to find out the appropriate ratio and to evaluate and analyze the internal curing effect of waste molecular sieves. Compressive strength, flexural strength, and dry shrinkage properties of mortar with different dosages of the molecular sieve are tested. The water release behavior of the molecular sieve in mortar is comprehensively analyzed combined with the desorption test of the molecular sieve. Results show that the compressive and flexural strength increase by 5% and 10%, respectively, and the drying shrinkage decrease by 6% when 10% of sand is replaced by a molecular sieve under the same total water content. The hydration behavior of the sample is characterized by a microcosmic test of paste. Thermogravimetric analysis is used to calculate the content of corresponding hydration products and quantitatively describe the hydration degree of the internal curing paste mixed with MS. Results show that the content of hydration products is improved by the addition of the molecular sieve, which provides a theoretical basis for the enhancement of mortar to a certain extent.
16 February 2026 in Construction and Building Materials
Metal centralizers suffer high frictional resistance, high self-weight, and severe pore shrinkage after perforation in deep, highly deviated, and horizontal wells. Targeting the performance demands of adhesive casing centralizers, this study uses epoxy resin as the matrix, introduces amino modification, and regulates inorganic filler composites to prepare an amino-modified epoxy resin composite centralizer material, followed by systematic property tests. The optimal formula of modified epoxy resin:curing agent:UR300 accelerator:amino-modified silica:silicon carbide:alumina is 100:10:1:1:35:20 and delivers superior comprehensive performance. Its compressive strength reaches 136.61 MPa with a Shore hardness of 92.32 HD, low linear expansion, and favorable thermal compatibility with steel casings. Hardness remains stable after 168 h of aging at 150 °C, and the material maintains low friction at ambient and elevated temperatures. After 30-day immersion in acidic, alkaline, and high-salinity fluids, its compressive strength retention exceeds 86% with a slight variation in volume and mass, while adhesion strength reaches 2.667 MPa at a pipe-wall roughness of 12.12 μm. Combining high strength, heat resistance, corrosion resistance, and strong adhesion, the material suits complex downhole conditions and supports the field application of resin composite centralizers.