An express method for assessing the effectiveness of lubricating compositions with nano-additives of various chemical compositions is proposed, and a joint analysis of experimental data on the changes in the value of wear and the level of damage to the surface layers of metallic friction pairs was performed. The variation in the current relative hardness of the sample’s surface, the variation in the current relative material damage level, the current value of wear, and the current level of the coefficient of friction were chosen as the key parameters to conduct a performance assessment. The level of material damage in the contact zone was determined using the parameters of the statistical law of hardness value scattering. Based on an analysis of data in the literature, it was observed that the structural changes occurring in metallic materials during long-term, cyclic, static, and frictional loading are correlated with changes in the statistical characteristics of the hardness scattering results. An experimental substantiation of the proposed method was carried out for steel-sliding friction pairs using lubricating compositions based on Greaseline Lithium BIO Rail 000 oil manufactured by AIMOL with nano-additives of copper, magnesium and aluminum alloys, graphite, and two grades of medium-carbon steel. According to the system of indicators presented in this research, the greatest efficiency (in terms of increasing the wear resistance of friction steel pairs) was achieved with lubricating compositions including nano-powder additives made of steel, which have lower hardness. For the friction experiments, where the determining factor was abrasive wear, such lubricants ensured minimal damage and wear to the friction surface, while the value of the friction coefficient was maintained at a level that is optimal for wheel–rail friction pairs.
24 December 2021 in Collection of scientific works of the State University of Infrastructure and Technologies series "Transport Systems and Technologies"
The paper presents modern concepts of the contact fatigue crack occurrence in the railhead. Numerical simulation of the contact interaction between rails and rolling stock wheels by finite elements method are presented. During the simulation, the problem was solved in elastic and elastic-plastic formulations. We considered R65 rail profile and standard railway wheels. The conditions for the rail–wheel interaction corresponded to train movement on the straight section of the track without slipping. The modern life assessment methodology involves the calculation of the material damage increment at each point of the element as the load varies over time, and subsequent summation of this damage. Upon reaching the ultimate value of the total damage, the structural element is believed to lose its load-carrying capacity, i.e. a crack is formed in it. Despite the substantial simplification of the real problem, the computational costs for the implementation of such methods for predicting the durability will be unnecessarily high. In this regard, we propose the simplified method of the durability calculation.
A new method is proposed for performance assessment of lubricating compositions based on industrial lubricants that contain nano-additives of different chemical composition for higher wear resistance of heavy-loaded steel friction pairs. The method is based on the joint analysis of the experimental data on the wear kinetics, change of the relative hardness, and damage in the surface layers of the metal of friction pairs. The level of structural damage to the materials in the contact zone is determined by using the statistical parameters of dispersion of the hardness values. The paper investigates the known experimental results of assessment of the level of damage to structural materials of various grades under the conditions of long-term, cyclic, static loading, and lubricated friction. It is demonstrated that the structural changes occurring in the materials during loading correlate to the changes in the statistical dispersion characteristics of hardness measurement results. Experimental substantiation of the method is carried out for steel friction pairs using lubricating compositions based on industrial oil Greaseline Lithium BIO Rail 000 by AIMOL and nano-additives of copper of M2 grade, magnesium alloy of MA2 grade, aluminum alloy of Al-Mg system, graphite of medium carbon steel grades, i.e. rail and industrial. Under system of indicators presented in the paper, the highest efficiency in terms of increase in the wear resistance of steel friction pairs is demonstrated by the lubricating composition based on industrial lubricant with the additive of nano-powder made of rail steel, as it provided the optimum value of friction coefficient, minimum damage and wear of friction surface.
12 December 2023 in Collection of scientific works of the State University of Infrastructure and Technologies series "Transport Systems and Technologies"
У статті проаналізовано відомі експериментальні результати оцінки ступеню пошкодження конструкційних матеріалів різних марок за умов довготривалого, циклічного, статичного навантаження та мастильного тертя. Показано, що структурні зміни, які відбуваються в матеріалах під час навантаження, корелюють зі змінами статистичних характеристик розсіювання результатів вимірювання твердості. Це дозволяє прогнозувати кінетику накопичення пошкоджень у матеріалах під час експлуатації, а отже, прогнозувати термін їх служби. Такий підхід є актуальним для розробки методів оцінки поточного стану та залишкового ресурсу конструкцій залізничного та інших транспортних галузей. Запропоновано використовувати цю методику для оцінки рівня пошкодження мікроструктури матеріалів у зоні контакту та його впливу на трибологічні характеристики металевих пар тертя. Запропоновано новий метод оцінки ефективності мастильних композицій на основі промислових мастил, які містять нанодобавки різного хімічного складу для підвищення зносостійкості сталевих важконавантажених пар тертя. Метод базується на спільному аналізі експериментальних даних щодо кінетики зношування, зміни відносної твердості та рівня пошкодженості поверхневих шарів металів пар тертя. Порушення структури матеріалів у зоні контакту визначають за допомогою статистичних параметрів розсіювання значень твердості. Методика апробована для сталевих пар тертя, де використовуються мастильні матеріали на основі індустріального масла та нанодобавок міді, магнієвих сплавів, графіту та двох марок середньовуглецевих сталей.