To understand the mechanical behavior of CRTS (China Railway Track System) II cement emulsified asphalt mortar (CA mortar), this study tested the compressive strength and flexural strength of CA mortar at different ages under varying water-to-cement ratios and dosages of water-reducing agent. Based on X-ray diffraction (XRD) and scanning electron microscopy (SEM) results, the hydration products and microstructure of CA mortar at different ages were analyzed. The main conclusions are as follows. As the water-to-cement ratio increases, the compressive strength and flexural strength of CA mortar generally exhibit a decreasing trend. The strength increases rapidly in the early stages, with the 7-day compressive strength reaching over 80% of the 28-day compressive strength, and the 7-day flexural strength reaching over 93% of the 28-day flexural strength. As the dosage of water-reducing agent increases, both the compressive strength and flexural strength of CA mortar first increase and then decrease, with a reasonable range of water-reducing agent dosage being between 0.2% and 1.0%, and 0.5% is most appropriate. The hydration reaction of CA mortar is nearly complete at 3 days, with the increase in ages, the cement hydration slows down due to the coating action of asphalt, and the strength no longer changes greatly. Hydration products are mainly Ettringite, which is the main source of strength of CA mortar. After the emulsified asphalt breaks, it adsorbs onto the hydration products and sand surfaces, gradually forming a continuous phase, which enhances the structural toughness of the CA mortar.
In the structure of composite pavement, the formation of voids beneath concrete panels poses significant risks to structural integrity and operational safety. Ground-Penetrating Radar (GPR) detection serves as an effective method for identifying voids beneath concrete pavement panels. This paper focuses on analyzing the morphological features of GPR echo signals. Leveraging the GprMax numerical simulation software, a numerical simulation model for void conditions in concrete pavement is established by setting reasonable pavement structure parameters, signal parameters, and model space parameters. The reliability of the numerical simulation model is validated based on field data from full-scale test sites with pre-fabricated voids. Various void conditions, including different void thicknesses, sizes, shapes, and filling mediums, are analyzed. The main conclusions of the study are as follows: the correlation coefficient between measured and simulated signals is above 0.8; a noticeable distinction exists between echo signals from intact and voided structures; signals exhibit similar phase and time delays for different void thicknesses and sizes but significant differences are observed in the A-scan signal intensity, the signal intensity, and the width of the B-scan signal; the impact of void shape on GPR echo signals mainly manifests in the variation of void thickness at different measurement points; and the relationship between the dielectric properties of the void-filling medium and the surrounding environment dictates the phase and time delay characteristics of the echo signal.