Self-healing materials are repairable and extend product lifetimes but are limited in application due to their mechanical properties such as low yield strength. Here, we examined the dynamic mechanical performance of an elastomeric polymer composite containing aramid nanofibers. These studies provided an economically feasible foundation to understand the reinforcement concentration and resultant mechanical properties that would result should aramid nanofibers be used to reinforce a self-healing polymer that requires complex synthesis methods and expensive reactants. The elastomeric polymer used was polycaprolactone containing various weight percent aramid nanofibers. Dynamic mechanical testing of these samples was performed using a split-Hopkinson pressure bar system that enabled quantification of polymer softening and aramid nanofiber reinforcement. Dynamic flow stress and strain rates were also calculated with these data. Crystallinity and thermal softening effects of solvent dissolution of polycaprolactone are explored to further characterize the performance of aramid nanofibers as a fiber in composite materials. Graphical abstract
Chitin is an abundant biopolymer, with 1–3 million tons potentially available annually from shellfish-processing waste, but remains underutilized because its insolubility in conventional solvents makes it difficult to process and functionalize. Herein, a three-step route to chitin adsorbents with interchangeable ligands is reported. Highly acetylated chitin was tosylated and converted to the C-6 azide, and amine- and hydroxyl-terminated ligands were attached to this common intermediate by the copper-catalyzed azide–alkyne cycloaddition (CuAAC) “click” reaction, yielding water-insoluble derivatives. Cu(II) adsorption to the adsorbents was evaluated using inductively coupled plasma optical emission spectrometry (ICP-OES analysis). Under standard conditions (pH 6.0, 4 h contact), amine- and alcohol-chitin adsorbed 30.1 ± 1.3 and 22.3 ± 1.9 mg Cu g−1, respectively, approximately 4.9- and 3.6-fold more than unmodified chitin. Isotherm data were well described by the Langmuir model, with apparent capacities of 37.4 and 25.7 mg g−1 at 4 h contact. The adsorbents could be regenerated with 7% (v/v) HCl, retaining 46% and 42% of their initial uptake after four cycles. The differences in derivatives’ uptakes are attributable to the identity of the grafted ligand, illustrating how the click route allows chitin adsorbents to be tailored through the choice of alkyne.