Mechanical properties are substantiated, that are the most vulnerable to maintenance material deterioration of under prolonged operating time, accompanied by intense damage. The opposite behavior of relative elongation and contraction indicates the intensity of scattered damage of the operated metal. Reducing the percentage reduction indicates operational metal embrittlement, as a result of strain hardening, which can serve as confirmation of the increase in hardness and microhardness. Fractographic analysis of failure mechanisms of steel 17G1S cut in the length and breadth of the pipe is implemented.
The areas of low frequency and corrosion fatigue for basic metal and welding joints of oil and gas pipelines have been determined on the basis of corrosion-fatigue test results. The most dangerous diapasons of the operation loadings were also determined. The present work also proposes the methodical approaches to the survivability prediction.
The processes of supplying natural gas are accompanied by significant losses. In this regard, the complex problem of minimizing losses and improving the efficiency of energy use is very relevant. Steel pipelines for transportation of oil and gas often cross the tracks or are located parallel to the lines of electric power transmission lines of alternating current. Most dangerous from the corrosive point of view of the combination of the chemical composition of the soil electrolyte and the vagal current density were established.