3 January 2024 in Welding in the World
Verified
Journal Article
Closed access
PDF file
TITamaki Ito
Tamaki Ito
KTKai Tomita
Kai Tomita
KTKoichi Taniguchi
Koichi Taniguchi
SISatoshi Igi
Satoshi Igi
MYMotomichi Yamamoto
Motomichi Yamamoto

4 September 2025 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
SYShaowei Yang
Shaowei Yang
TITamaki Ito
Tamaki Ito
KMKeita Marumoto
Keita Marumoto
KSKenji Shinozaki
Kenji Shinozaki
MYMotomichi Yamamoto
Motomichi Yamamoto

5 July 2023 in Welding International
Verified
Journal Article
Closed access
TITamaki Ito
Tamaki Ito
JCJeong-Won Choi
Jeong-Won Choi
MYMotomichi Yamamoto
Motomichi Yamamoto
KTKoichi Taniguchi
Koichi Taniguchi
YOYasuaki Okita
Yasuaki Okita
HMHiroshi Matsuda
Hiroshi Matsuda

20 November 2025 in Metals
Verified
Journal Article
Open access
PDF file
TITamaki Ito
Tamaki Ito
SYSHAOWEI YANG
SHAOWEI YANG
KMKeita Marumoto
Keita Marumoto
KSKenji Shinozaki
Kenji Shinozaki
MYMotomichi Yamamoto
Motomichi Yamamoto
In welding solidification, the morphology of residual liquid in the solid–liquid coexistence region affects the susceptibility to solidification cracking because this cracking is due to localized shrinkage strain in the residual liquid. Therefore, it is important to observe the residual liquid state during solidification in detail to elucidate the occurrence of solidification cracking. In this study, a high-magnification in situ observation system was developed by combining an optical microscope and a high-speed camera. This system enables continuous, high-magnification, and high-resolution observation of welding solidification, because the objective lens of a microscope is attached to a high-speed camera. Laser welding solidification of stainless steel sheets was observed using this system and the morphology of residual liquid was visualized with higher magnification and higher definition than previous observation methods. Compared with a high-magnification image and quenched solidification microstructure, the residual state of the liquid phase during solidification could be observed in detail and dynamically. Additionally, the difference in solidification between two types of stainless sheets could be observed with high magnification in situ at one point. Finally, the combination of the observation results from this system and a high-temperature ductility curve revealed the relationship between the morphology of residual liquid and solidification cracking susceptibility.

27 March 2026 in Materials & Design
Verified
Journal Article
Open access
SYShaowei Yang
Shaowei Yang
TITamaki Ito
Tamaki Ito
GLGuoliang Liu
Guoliang Liu
ZHZiyang Hu
Ziyang Hu
KMKeita Marumoto
Keita Marumoto
MYMotomichi Yamamoto
Motomichi Yamamoto

31 August 2023 in Research Square
Verified
Preprint
Open access
PDF file
TITamaki Ito
Tamaki Ito
KTKai Tomita
Kai Tomita
KTKoichi Taniguchi
Koichi Taniguchi
SISatoshi Igi
Satoshi Igi
MYMotomichi Yamamoto
Motomichi Yamamoto
When steels and aluminum alloys are joined by normal welding, brittle intermetallic compounds (IMC) are generated at the interface, which causes a decrease in joint strength. Dissimilar steel/aluminum alloy joints formed via hot-wire laser brazing can stably suppress IMCs, as elucidated by visualization during brazing and cross-sectional imaging of fabricated joints. In addition, the effects of various coatings on steel plates were investigated by comparing joint cross-sections and interfaces. Zn (galvanized, galvannealed) layers, flux, and a molten pool prevented direct laser-beam irradiation of the steel surfaces. A high brazing speed could enable a high cooling rate, creating a very low peak temperature of the steel and suppressing IMC formation. The galvanized Zn coating also prevented direct contact of the aluminum alloy with the steel surface. Thus, the galvanized steel suppressed IMC formation more than non-coated steel. Because a Fe-Zn alloy coating layer was a source of Fe for IMC formation, a thicker IMC was generated on galvannealed steel.