The large-scale coke oven is a developing trend in coking technology, and the influence of the industrial coke oven size on the quality of metallurgical coke needs to be revealed. Under the same raw coals and blending ratios, metallurgical cokes were obtained from top-loading coke ovens with carbonization chamber heights of 6 and 7 m, respectively. The macroscopic quality and microstructure of the refined metallurgical cokes were comprehensively tested. The results showed that the conventional cold and thermal strength indexes of Coke-7m were better than those of Coke-6m. The comprehensive thermal strength at multiple temperatures further showed that the thermal strength advantage of Coke-7m was mainly manifested at low temperatures (1050 and 1100 °C) or a high temperature (1300 °C), where the solution-loss reaction mode of coke tended to be the “uniform reaction model” or “unreacted core model”. At medium temperatures, the solution-loss reaction mode tended to be the “gradient reaction model”, which had a greater destructive effect on the thermal strength of coke. At this time, the thermal strengths of the two cokes were close. Microstructure characterization revealed that industrial coke oven size mainly affected the carbon structure of coke but had little effect on pore structure. The advantage of Coke-7m regarding carbon structure is an important reason for its superior macroscopic quality compared to Coke-6m.
The quality of coke is to some extent closely related to the technological properties of coking coals due to the differences in chemical structure of cokin
Hydrogen-rich blast furnaces require the use of highly reactive coke due to their lower furnace temperature. In addition, a hydrogen-rich blast furnace contains a large amount of water vapor. We investigated the reaction behavior of highly reactive briquetting coke prepared from low-rank coal as the main raw material under a CO2 + H2O atmosphere. The reaction behavior and postreaction compressive strength of coke at different H2O contents were examined. The changes in microcrystalline structure, functional groups, apparent porosity, micron pore structure, nitrogen and carbon dioxide adsorption properties of coke before reaction and after gasification reaction at different H2O contents were investigated. Compared with traditional coke, briquetting coke not only has high reactivity at different H2O contents but also high compressive strength after reaction. The reaction of briquetting coke under a CO2 + H2O atmosphere was significantly controlled by surface reactions.