The silico-ferrite of calcium and aluminum (SFCA) is a significant crystalline phase that bonds in high basicity sinter. Al2O3 and SiO2 play an important role in the formation of SFCA in the Fe2O3–CaO–SiO2–Al2O3 system, but the effect mechanism of Al2O3 and SiO2 on the formation of SFCA is unclear. To investigate this effect, sintering experiments were carried out with different temperatures and different times. It was found that the reaction of Al2O3 with CaFe2O4 (CF) as an initial product was easier to form during the calcium iron aluminum oxide (CFA) than that of SiO2 with CF to form SFC. This was due to the former directly forming to CFA while the latter initially formed Ca2SiO4 (C2S) and Ca2.5Fe15.5O25, and then SFC. It was also observed that when Al2O3 and SiO2 existed simultaneously, the Al2O3 initially reacted with CF to form CFA at 1100 °C, while the SiO2 participated in the formation of SFCA at 1150 °C without the formation of SFC. Moreover, it was understood that these were different effects in that the Al2O3 promoted the transformation from the orthorhombic crystal system to the triclinic crystal system, while the SiO2 dissolved into CFA to form the SFCA phase when Al2O3 existed.
The large-scale coke oven is a developing trend in coking technology, and the influence of the industrial coke oven size on the quality of metallurgical coke needs to be revealed. Under the same raw coals and blending ratios, metallurgical cokes were obtained from top-loading coke ovens with carbonization chamber heights of 6 and 7 m, respectively. The macroscopic quality and microstructure of the refined metallurgical cokes were comprehensively tested. The results showed that the conventional cold and thermal strength indexes of Coke-7m were better than those of Coke-6m. The comprehensive thermal strength at multiple temperatures further showed that the thermal strength advantage of Coke-7m was mainly manifested at low temperatures (1050 and 1100 °C) or a high temperature (1300 °C), where the solution-loss reaction mode of coke tended to be the “uniform reaction model” or “unreacted core model”. At medium temperatures, the solution-loss reaction mode tended to be the “gradient reaction model”, which had a greater destructive effect on the thermal strength of coke. At this time, the thermal strengths of the two cokes were close. Microstructure characterization revealed that industrial coke oven size mainly affected the carbon structure of coke but had little effect on pore structure. The advantage of Coke-7m regarding carbon structure is an important reason for its superior macroscopic quality compared to Coke-6m.
This research aimed to investigate the production of ferro coke with high strength by cold pressing without adding binder, to meet the requirements of the metallurgical industry and avoid the environmental pollution problems caused by the hot pressing process. The effects of pressure and proportion of iron ore powder on the preparation of ferro coke from a weakly caking coal and a strongly caking coal were studied. The results show that when no binder is added, the ferro coke made from weakly caking coal has the highest compressive strength of 5.13 KN, while the ferro coke made from strongly caking coal has the highest compressive strength of 4.93 KN.The relationship between the strength of ferro coke and the rate of dissolution loss was studied, and it was found that weakly caking coal produced under high forming pressure had good performance.
Hydrogen-rich blast furnaces require the use of highly reactive coke due to their lower furnace temperature. In addition, a hydrogen-rich blast furnace contains a large amount of water vapor. We investigated the reaction behavior of highly reactive briquetting coke prepared from low-rank coal as the main raw material under a CO2 + H2O atmosphere. The reaction behavior and postreaction compressive strength of coke at different H2O contents were examined. The changes in microcrystalline structure, functional groups, apparent porosity, micron pore structure, nitrogen and carbon dioxide adsorption properties of coke before reaction and after gasification reaction at different H2O contents were investigated. Compared with traditional coke, briquetting coke not only has high reactivity at different H2O contents but also high compressive strength after reaction. The reaction of briquetting coke under a CO2 + H2O atmosphere was significantly controlled by surface reactions.
5 July 2025 in Applied Biochemistry and Biotechnology