SiC-coated C/C composites with mechanical damage were repaired by the heat treatment method and slurry painting–preoxidation. The effects of different process parameters on the microstructure, interface bonding and oxidation resistance of Si-SiC repair coatings at 1773 K for 10 h were studied. The results show that the repair coating is tightly bonded to the original coating and the C/C substrate, and there is no obvious interface. Under the optimal parameters, the weight reduction in the repaired specimen merely amounted to 0.32% subsequent to oxidation at 1773 K for 10 h, and the mass loss was 74.79% lower than that of the damaged specimen, being proximate to that of the intact specimen. The objective of this work lies in achieving a greater density of the coating within the repair zone by manipulating the diverse powder ratios and preoxidation temperatures in the repair slurry, thereby safeguarding the C/C composite material against oxidation during its service. It offers a convenient and highly efficient approach for the repair of coatings with substantial size defects, significantly prolonging the service life of the material.
The effect of covalent element addition on the magnetic and magnetocaloric properties of ferrimagnetic Gd60Co20Fe20 amorphous alloy was studied. Particularly, the co-doping of B and Si promoted the magnetocaloric performance (with a larger magnetic entropy change |ΔSM| at higher working temperature) of the initial Gd60Co20Fe20 amorphous alloy. This is possibly ascribed to the modified magnetic transition behavior. Additionally, the broadened magnetocaloric effect with |ΔSM| of 2.25 J kg−1 K−1 at 222.5 K under a magnetic field change of 0–2 T and high relative cooling power of 396.0 J kg−1 were obtained for (Gd0.6Co0.2Fe0.2)95B2Si3. These properties reveal that the material could be a good candidate as a magnetic refrigerant suitable for active magnetic refrigerators.