Microcellular injection molding technology (MuCell®) using supercritical fluid (SCF) as a foaming agent offers many advantages, such as material and energy savings, low cycle time, cost-effectiveness, and the dimensional stability of products. MuCell® has attracted great attention for applications in the automotive, packaging, sporting goods, and electrical parts industries. In view of the environmental issues, the shoe industry, particularly for midsole parts, is also seriously considering using physical foaming to replace the chemical foaming process. MuCell® is thus becoming one potential processing candidate. Thermoplastic polyurethane (TPU) is a common material for molding the outsole of shoes because of its outstanding properties such as hardness, abrasion resistance, and elasticity. Although many shoe manufacturers have tried applying Mucell® processes to TPU midsoles, the main problem remaining to be overcome is the non-uniformity of the foaming cell size in the molded midsole. In this study, the MuCell® process combined with gas counter pressure (GCP) technology and dynamic mold temperature control (DMTC) were carried out for TPU molding. The influence of various molding parameters including SCF dosage, injection speed, mold temperature, gas counter pressure, and gas holding time on the foaming cell size and the associated size distribution under a target weight reduction of 60% were investigated in detail. Compared with the conventional MuCell® process, the implementation of GCP technology or DMTC led to significant improvement in foaming cell size reduction and size uniformity. Further improvement could be achieved by the simultaneous combination of GCP with DMT, and the resulting cell density was about fifty times higher. The successful possibility for the microcellular injection molding of TPU shoe midsoles is greatly enhanced.
Microcellular injection molding technology (MuCell) using supercritical fluid (SCF) as a foaming agent is one of the important green molding solutions for reducing the part weight, saving cycle time, and molding energy, and improving dimensional stability. In view of the environmental issues, the successful application of MuCell is becoming increasingly important. However, the molding process encounters difficulties including the sliver flow marks on the surface and unstable mechanical properties that are caused by the uneven foaming cell sizes within the part. In our previous studies, gas counter-pressure combined with dynamic molding temperature control was observed to be an effective and promising way of improving product quality. In this study, we extend this concept by incorporating additional parameters, such as gas pressure holding time and release time, and taking the mold cooling speed into account to form a P(pressure)-T(temperature) path in the SCF PT diagram. This study demonstrates the successful control of foaming cell size and uniformity in size distribution in microcellular injection molding of polystyrene (PS). A preliminary study in the molding of elastomer thermoplastic polyurethanes (TPU) using the P-T path also shows promising results.
During an injection molding process, different parts of the molded material are subjected to various thermal–mechanical stresses, such as variable pressures, temperatures, and shear stresses. These variations form different pressure–temperature paths on the pressure–volume–temperature diagram. If these paths cannot converge at a specific target volume value during ejection, it often leads to different levels of shrinkage and associated warping, which pose a significant challenge for molders during mold trials and part quality control. The situation is particularly complicated when molding crystalline polymers because the degree of crystallinity depends on the processing conditions and may vary across different locations. In this study, we propose an innovative and practical approach to improving part shrinkage when molding crystalline polymers. For the first time, we utilized melt temperature profile monitoring rather than the previous mold temperature measurement to detect the crystallization process and determine the time taken to complete the crystallization at different melt and mold temperatures. In addition, we used response surface methodology to build a crystallization time prediction model. The feasibility of the prediction model was verified by determining the warpage of parts molded at various cooling times. Based on this model, we varied the packing pressure, packing time, and melt temperatures to determine the correlation with part shrinkage. Through regression analysis, the time-averaged solidification pressure values can accurately control part shrinkage. Two prediction models provide reasonable accuracy and efficiency for part shrinkage control, as demonstrated by subsequent verification experiments.
Microcellular injection molding (MuCell®) using supercritical fluid (SCF) as a foaming agent to achieve weight reduction has become popular in carbon emission reduction. In the typical MuCell® process, SCF N2 is commonly used. Although SCF CO2 exhibits high solubility and can achieve a high weight reduction, controlling the foaming is not easy, and its foaming cells are usually larger and less uniform, which limits its industrial application. Our previous studies have shown that gas counter pressure (GCP) can improve the foaming quality effectively. Here, we investigated whether or not the CO2 SCF foaming quality could be improved, and weight reduction was achieved for polycarbonate (PC) material. This is quite important for the electronics industry, in which most of the housing for devices is made of PC materials. MuCell® was subjected to molding experiments using the parameters of the SCF dosage, melt temperature, mold temperature, and injection speed. The results revealed that using CO2 gas for the PC material can reduce the size of microcellular cells to 40 µm and increase the cell densities to 3.97 × 106 cells/cm3. Using GCP significantly improved the microcellular injection-molded parts by reducing the cell size to 20.9 µm (a 45.41% improvement) and increasing the cell density to 8.04 × 106 cells/cm3 (a 102.48% improvement). However, implementing GCP may slightly decrease the target weight reduction. This study reveals that microcellular injection molding of PC parts using SCF CO2 can achieve high-quality foaming and reduce the weight by about 30%.