The Johnson–Cook model is widely used because of its ability to meet the simulation material requirements in various situations. However, under different working conditions, the accuracy of the model may have errors. In this work, based on Abaqus (Abaqus R2022 Education Edition, Dassault Systèmes, Paris, France) simulation software, Johnson–Cook (JC) constitutive model parameters and compression parameters were selected to simulate the improvement of surface roughness during the ball milling of a 7075-T651 aluminum alloy. In the numerical simulation of ball polishing, the changes in the residual stress field when the Johnson–Cook parameters change are analyzed. By comparing the numerically simulated residual stress fields under the JC parameters calculated at different strain rates, a set of parameters that agrees with the experimental values is selected. The results show that the residual stresses are in line with the experimental values when the strain rate is 10−4s −1. The changes in roughness corresponding to the selected parameters are analyzed. The results indicate that the simulated trend of roughness variation is consistent with the experimental values, and the optimal surface roughness value under a static pressure of 300 N is obtained.
This study systematically revealed the synergistic effects of laser power, cladding speed, and substrate diameter on the dilution rate and hardness of iron-based alloy coatings on the surface of 45 steel through the integration of finite element simulation, elemental migration analysis, and response surface methodology (RSM). The experiments showed that when the substrate diameter was greater than 50 mm, the coupling effect of thermal diffusion retardation and molten pool expansion caused a nonlinear surge in the dilution rate. The growth rate of the molten pool depth increased by 46% (from 0.28 to 0.41 μm), and the melting volume of the substrate expanded by 1.7 times. The dilution rate reached 15.6%–31.7% through a dual-regulation mechanism involving energy density (1.43–3.75 J/mm2) and substrate diameter (30–60 mm), with a significant hardness demarcation of 343–738 HV. Substrates with a small diameter (30 mm) achieved a peak hardness of 738 HV at an energy density of 2.14 J/mm2 through ultra-fast cooling (>1.5 × 104 K/s), while those with a large diameter (60 mm) exhibited a hardness drop to 426.5 HV due to grain coarsening. The multi-method integrated model constructed in this study achieved a dilution rate prediction error of less than 5% (R2 = 0.9775), with a prediction deviation of less than 2% under extreme parameters (diameter of 55 mm and power of 4800 W). The study proposed an optimized process window with a substrate diameter of 42–57 mm and an energy density of 1.43–2.14 J/mm2, providing a physically mechanism-driven intelligent parameter design strategy for laser cladding repair of shaft parts.