The ChCl·1.5CF3O3S DESs is synthesized by stirring at the room temperature. The high efficient desulfurizative system using ChCl·1.5CF3O3S DESs as extractant and catalyst, H2O2 as oxidant with small amount of H2O2 (an O/S molar ratio of 6) and the low temperature (40 °C).
Propionic acid-based deep eutectic solvents (C3H6O2/X ZnCl2, X from 0.1 to 0.6) were synthesized by stirring a mixture of propionic acid and zinc chloride at 100 °C.
The n %-SnO 2 /SiO 2 ( n = 2, 4, 6) supported catalyst was prepared by the sol–gel and calcination method. Compared with the traditional impregnation method, the catalyst prepared by sol–gel method has higher oxidative desulfurization activity.
N,N-Dimethylformamide hydrochloric acid/XMCln ([HDMF]Cl/XMCln, M = Zn or Fe, n = 2 or 3) was synthesized by stirring the mixture of [HDMF]Cl and metal chloride. [HDMF]Cl-based DES was characterized by FT-IR spectroscopy, ESI-MS and 1H-NMR spectroscopy. The oxidative desulfurization activity was investigated using [HDMF]Cl/0.2FeCl3 and [HDMF]Cl/ZnCl2 as the extractant and catalyst, and hydrogen peroxide (H2O2) as the oxidant. The desulfurization rate can reach up to 98.08% and 99.2% for DBT using [HDMF]Cl/0.2FeCl3 and [HDMF]Cl/ZnCl2, respectively. After recycling for 7 times, the removal rate of DBT still can reach more than 97%.
12 April 2016 in Research on Chemical Intermediates
The ultra-deep desulfurization of fuel oil has become inevitable for environmental protection. Here, CoWO4/g-C3N4 was used as a catalyst, H2O2 as an oxidant, and 1-ethyl-3-methylimidazolium ethylsulfate ([EMIM][EtSO4], IL) as an extractant for the oxidative desulfurization of model oil. Scanning electron microscopy, FT-IR spectroscopy, N2 adsorption isotherms, and X-ray diffraction were used to confirm the morphology, structure, and properties of the catalysts. The influence of calcination temperature, loading dose of cobalt, amount of H2O2, reaction temperature, and other parameters were investigated. The removal rate of sulfide in model oil could reach 92.9 % at 80°C in 180 min under the optimal operation conditions (V(oil) = 5 mL, T = 80°C, m(catalyst) = 0.03 g, V(H2O2) = 0.4 mL, t = 180 min, V(IL) = 1.0 mL). In addition, the catalyst was reused five times with no significant reduction in the catalytic activity.