The thermal and plasma-enhanced atomic layer deposition (ALD) growth of titanium oxide using an alkylamine precursor – tetrakis(dimethylamino)titanium (TDMAT) – was investigated. The surface species present during both the precursor and co-reactant pulse were studied with in situ reflection mid-IR spectroscopy (FTIR) and in vacuo X-ray photoelectron spectroscopy (XPS). The thermal process using H2O vapor proceeds through a typical ligand exchange reaction mechanism. The plasma-enhanced ALD processes using H2O-plasma or O2-plasma exhibit an additional decomposition and combustion reaction mechanism. After the plasma exposure, imine (NC) and isocyanate (NCO) surface species were observed by in situ FTIR. In addition, nitrites (NOx) were detected using in vacuo XPS during the O2-plasma process. This study presents the importance of the use of in situ FTIR and in vacuo XPS as complementary techniques to learn more about the ALD reaction mechanism. While in situ FTIR is very sensitive to changes of chemical bonds at the surface, exact identification and quantification could only be done with the aid of in vacuo XPS.
In this work, three atomic layer deposition (ALD) approaches are used to deposit an Al2O3 gate insulator on n-GaN for application in vertical GaN power switches: thermal ALD (ThALD), plasma-enhanced ALD (PEALD), and their stacked combination. The latter is a novel method to yield the most ideal insulating layer. Also, the influence of an in situ NH3 or H2 plasma pre-treatment is studied. Planar MIS capacitors are used to investigate the electrical properties and robustness of the gate insulators. In vacuo x-ray photoelectron spectroscopy (XPS) is used to study the changes in chemical composition after every surface treatment. XPS shows that all plasma pre-treatments efficiently remove all carbon contamination from the surface, but only NH3 plasma is observed to additionally remove the native oxide from the n-GaN surface. The water precursor step in the ThALD process does not completely remove the CH3 ligands of the trimethylaluminum precursor step, which might electrically be associated with a reduced forward bias robustness. The O2 plasma step in the PEALD process is associated with the removal of carbon and a tremendous increase of the O content in the GaN surface region. Electrically, this strongly correlates to an enhanced forward bias robustness and an increased forward bias hysteresis, respectively. The ThALD/PEALD stack method mitigates the shortcomings of both ALD processes while maintaining its advantages. Electrical measurements indicate that the stack method alongside NH3 plasma pretreatment provides the best characteristics in terms of hysteresis, threshold voltage, forward bias robustness, and interface trap density of states.
Alucones are one of the best-known films in the Molecular Layer Deposition (MLD) field. In this work, we prove that alucone/Al 2 O 3 nanolaminate synthesis can be successfully performed by alternating alucone MLD growth with static O 2 plasma exposures.
5 December 2022 in Semiconductor Science and Technology
The chemical, physical and electrical properties and the robustness of post metallization annealed Al2O3 atomic layers deposited on n-type GaN are investigated in this work. Planar metal insulator capacitors are used to demonstrate a gate-first with following ohmic contacts formation at elevated temperature up to 600 °C process flow. X-ray photoelectron spectroscopy indicates that no new bonds in the Al2O3 layer are formed due to exposure to the elevated annealing temperature. X-ray diffraction measurements show no crystallization of the oxide layer. Atomic force microscopy shows signs of degradation of the sample annealed at 600 °C. Electrical measurements indicate that the elevated annealing temperature results in an increase of the oxide depletion and the deep depletion capacitances simultaneously, that results in a reduction of the flat band voltage to zero, which is explained by fixed oxide charges curing. A forward bias step stress capacitance measurement shows that the total number of induced trapped charges are not strongly affected by the elevated annealing temperatures. Interface trap density of states analysis shows the lowest trapping concentration for the capacitor annealed at 500 °C. Above this temperature, the interface trap density of states increases. When all results are taken into consideration, we have found that the process thermal budget allows for an overlap between the gate oxide post metallization annealing and the ohmic contact formation at 500 °C.