The forming limit behaviour of AA6013-T6 aluminium alloy sheet was characterized under isothermal conditions at room temperature (RT) and 250°C using limiting dome height (LDH) tests. Full field strain measurements were acquired throughout testing using in situ stereoscopic digital image correlation (DIC) techniques. Limit strain data was generated from the resulting full field strain measurements using two localized necking criteria: ISO12004- 2:2008 and a time and position dependent criterion, termed the "Necking Zone" (NZ) approach in this paper, introduced by Martinez-Donaire et al. (2014). The limit strains resulting from the two localization detection schemes were compared. It was found that the ISO and NZ limit strains at RT are similar on the draw-side of the FLD, while the NZ approach yields a biaxial major limit strain 14.8% greater than the ISO generated major limit strain. At 250°C, the NZ generated major limit strains are 31-34% greater than the ISO generated major limit strains for near uniaxial, plane strain and biaxial loading conditions, respectively. The significant variance in limit strains between the two methodologies at 250°C highlights the need for a validation study regarding warm FLC determination.
21 September 2018 in IOP Conference Series: Materials Science and Engineering
This work examines the nature of the strain distributions and limit stains during die quenching of a 7000-series aluminum alloy sheet. Forming limit experiments using limiting dome height (LDH) specimens were performed under plane-strain loading conditions using a 100 mm hemispherical Nakazima punch. Strains were measured using in situ stereoscopic digital image correlation (DIC). Two forming processing routes were examined: (i) an intermediate quench and form (IQF) processing route in which the LDH coupons were solutionized, quenched to a preset temperature, and isothermally formed and (ii) a die-quench (DQ) process where the LDH coupons were solutionized, and quenched and formed simultaneously with room temperature (RT) tooling under non-isothermal conditions. The DQ processing route was devised to understand the formability of the alloy under practical die-quenching conditions, while the IQF route was meant to understand the influence of temperature on the formability of the material. The DQ processing route exhibited the best formability from a localization standpoint; however, it was found that at deformations in excess of 0.5 major true strain, an orange-peel defect was present. The IQF process with room temperature tooling may be comparable to a W-temper forming operation. For these conditions, significant Portevin-Le-Chatelier (PLC) bands were present and the formability was approximately 75% less than for the DQ process. All formability results are summarized and a discussion of the interpretation of forming limits under the diffuse necking conditions associated with elevated temperature forming is presented.
12 June 2023 in Journal of Materials Engineering and Performance
Warm forming has been shown to be an effective way to increase the formability of various aluminum sheet alloys. If applied to precipitation hardenable alloys, aging and/or coarsening may occur during heating and/or forming processes. As such, there is a potential to leverage the warm forming process to artificially age precipitation hardenable alloys. In this study, the aging characteristics of a pre-aged Al-Mg-Si-Cu alloy (designated AA6013-PA and comprising a 4 h, 100 °C pre-aging cycle following solutionization) were examined using: (i) room temperature tensile and (ii) bendability experiments, as well as (iii) elevated temperature tensile and formability experiments in the temperature range of 220-280 °C. In the pre-aged condition, the alloy exhibited very high work hardening, elongation and bendability. It was found that T6-like properties can be obtained with short duration secondary aging of the AA6013-PA starting temper (410 s at 235 °C), followed by a paint bake cycle (30 min at 177 °C). In such heavily aged conditions, the bendability is found to be moderate and consistent with a T6 temper. Bendability of the pre-aged alloy is shown to be enhanced by reducing the extent of aging, which may be beneficial for applications requiring energy absorption during crash, for example. In the pre-aged condition, AA6013 displayed a 55% improvement in room temperature formability, relative to the T6 condition, for near plane-strain loading using a Nakazima punch, although neither temper exhibited formability improvements through warm forming. The aging kinetics of AA6013-PA were determined from mechanical test data and used to calibrate an aging kinetics model. A strong obstacle model was used to relate precipitation state to yield strength, for artificial aging in the range 220-280 °C. The incremental strength increase due to exposure to an automotive paint cure cycle was also modeled and found to yield accurate results. Warm deformation, as well as room temperature deformation, were shown to enhance the paint bake response of the alloy, reducing the time to the peak aged condition by up to 14% for artificial aging at 177 °C.
Despite advancements in the characterization of forming limit curves (FLCs) with the development of stereoscopic digital image correlation (DIC), there is still uncertainty in the accuracy of the limit strains, especially in forming operations with out-of-plane bending. The ISO12004-2:2008 standard offers a standardized approach to FLC determination but is not without limitations and is not always applicable to new materials and forming processes (e.g., warm forming, hot stamping). In the present work, a physically based limit strain detection technique is developed, termed the Enhanced Curvature Method (ECM), based on the sheet surface curvature evolution at the onset of necking in sheet formability testing. The ECM is applied to the characterization of 1.1 mm AA5182-O sheet using Marciniak, Nakazima, and stretch–bend characterization tests, and its limit strains are compared with those from the linear best-fit (LBF) local strain-rate approach and the ISO-12004 standard. The ECM considers the physical nature of necking in sheet forming with the aid of thresholds defined in terms of an imperfection metric analogous to the well-known Marciniak–Kuczynski (MK) imperfection factor. By quantifying the evolution of necking, FLCs of different safety margins can be readily generated, enabling a more intuitive selection for the factor of safety. For lower and upper ECM thresholds, the Marciniak plane strain limiting strain was determined to lie between 0.173 and 0.198, respectively, which is comparable to the analytical prediction of 0.194 and in general agreement with the published literature for AA5182-O. Similar plane strain limits were obtained using the ISO and LBF methods with values of 0.188 and 0.208, respectively. The same rankings in limit strain values between methods were observed for plane strain loading in Nakazima and stretch–bend tests.