Chunmin Yang

Dr. Chunmin Yang


Research Focus & Metrics

Academic Career Length

12Years (2015-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
26 September 2015 in Journal of Applied Polymer Science
Verified
Journal Article
Closed access
PDF file
XKXueqin Kang
Xueqin Kang
WZWei Zhang
Wei Zhang
CYChunmin Yang
Chunmin Yang

13 January 2025 in Lubricants
Verified
Journal Article
Open access
PDF file
CYChunmin Yang
Chunmin Yang
JZJunhua Zhang
Junhua Zhang
HYHonglin Yue
Honglin Yue
XKXueqin Kang
Xueqin Kang
Ultrahigh-molecular-weight-polyethylene (UHMWPE) is extensively applied to make bone and cartilage implants in the field of biomaterial application. UHMWPE matched with a metal or ceramic component withstands the long-term effect of cyclic stress, which induces UHMWPE serious wear, and affects the service life of the artificial joint. This investigation focuses on the influence of pores on the mechanical and tribological property of UHMWPE. The porosity, crystallinity, yield strength, tensile strength, hardness, compression yield strength, creep resistance, wettability, friction performance, and wear mechanism of solid and porous UHMWPE were evaluated and compared. The research results indicated that the pore had a remarkable influence on the mechanical, friction, and wear property of UHMWPE. The porosity of porous UHMWPE was 29.7% when 50 wt. % sodium chloride (NaCl) was added and the pore size was about 200 μm. The crystallinity, hardness, creep resistance, strength, and elongation decreased after NaCl was added and dissolved. However, the yield strength in the tensile and compression test was closer to that of the natural cartilage. The friction coefficient and wear loss of porous UHMWPE were higher than that of solid UHMWPE in dry conditions, but these values of porous UHMWPE were lower than that of solid UHMWPE in the calf serum lubrication condition. The main wear mechanism of porous and solid UHMWPE was abrasive. The lubricity of calf serum reduced wear surface scratches and furrows, especially for porous UHMWPE.

5 September 2024 in Materials
Verified
Journal Article
Open access
PDF file
YYYonghao Yu
Yonghao Yu
DZDapeng Zhou
Dapeng Zhou
LQLei Qiao
Lei Qiao
PFPeizhong Feng
Peizhong Feng
XKXueqin Kang
Xueqin Kang
CYChunmin Yang
Chunmin Yang
Co-Al porous materials were fabricated by thermal explosion (TE) reactions from Co and Al powders in a 1:1 ratio using NaCl as a space retainer. The effects of the NaCl content on the temperature profiles, phase structure, volume change, density, pore distribution and antioxidation behavior were investigated. The results showed that the sintered product of Co and Al powders was solely Co-Al intermetallic, while the final product was Co4Al13 with an abundant Co phase and minor Co2Al5 and Co-Al phases after added NaCl dissolved out, due to the high Tig and low Tc. The open porosity of sintered Co-Al compound was sensibly improved to 79.5% after 80 wt.% of the added NaCl dissolved out. Moreover, porous Co-Al intermetallic exhibited an inherited pore structure, including large pores originating from the dissolution of NaCl and small pores in the matrix caused by volume expansion due to TE reaction. The interconnected large and small pores make the open cellular Co-Al intermetallic suitable for broad application prospects in liquid–gas separation and filtration.

1 July 2025 in Scientific Reports
Verified
Journal Article
Open access
PDF file
JZJunhua Zhang
Junhua Zhang
DZDapeng Zhou
Dapeng Zhou
LQLei Qiao
Lei Qiao
YYYonghao Yu
Yonghao Yu
CYChunmin Yang
Chunmin Yang
XKXueqin Kang
Xueqin Kang
Porous Co-Al compounds with different Co/Al molar ratios were synthesized by thermal explosion (TE) reaction under 1 °C/min heating rate. Volume expansion behavior, microstructure, phase composition and antioxidation performance of Co-Al sintered specimens were researched and compared. Results showed that the sintered specimens under 1 °C/min heating rate were better to maintain the original shape, had an obvious dimension and volume expansion behavior, higher open porosity, superior antioxidation performance and the oxidation time to stable state was shorter compared with the intermetallics fabricated under 10 °C/min heating rate. The TE compact with molar ration of Co: Al = 2:9 had the largest volume expansion ratio of 109.6%, the highest open porosity of 52.8% and the lowest density of 1.47 g cm− 3 in all the Co/Al molar ratios compounds experimented in this study.