A high-pressure water jet can break rock efficiently, which is of great potential to overcome the problems of a tunnel boring machine (TBM) in full-face hard rock tunnel digging, such as low digging efficiency and high disc cutter wear rate. Therefore, this paper presented a new tunneling method that is a TBM coupled with a high-pressure water jet. The rock failure mechanism under the coupled forces of a disc cutter and water jet was analyzed at first. Then, the finite element method (FEM) and smoothed particle hydrodynamics (SPH) method were used to establish a numerical model of rock broken by the disc cutter and water jet. Effects of parameters on rock breaking performance were studied based on the numerical model. Moreover, an experiment of the water jet cutting marble was carried out to verify the reliability of the numerical simulation. Results showed that the high-pressure water jet can increase the TBM digging efficiency and decrease the forces and wear rate of the disc cutter. The optimum nozzle diameter is 1.5 mm, while the optimum jet velocity is 224.5 m/s in this simulation. The results can provide theoretical guidance and data support for designing the most efficient system of a TBM with a water jet for digging a full-face hard rock tunnel.
Cu/Al composite plate was manufactured by underwater explosive welding method. The interface characteristics and mechanical properties of Cu/Al composite plate were evaluated and analyzed through phased array ultrasonic inspection, microstructure, uniaxial tensile test, three-point bending test, tensile shearing test and microhardness test. The results showed that the welding of thin Cu and Al plates is achieved by underwater explosive welding, with a Cu plate thickness of only 0.5 mm. A well bonded interface between Cu and Al plate is obtained, at a detonation velocity of 4 000 m/s, when the distance between Cu foil and Al plate is 0.2 mm. There are wavy fusion zones at the bonding interface of Cu/Al composite plate. No delamination or cracks are found at the bonding interface between Cu and Al during tensile and bending tests, and local cracking only occurs at the necking part in the tensile test due to severe deformation. The tensile strength and minimum tensile shearing strength of Cu/Al composite plate reaches 133 and 72.9 MPa, respectively. The hardness values of fusion zone, Cu and Al at the interface reach 385, 135 and 52 HV, respectively. The increase in hardness of Cu and Al near the interface is mainly caused by severed deformation induced by intense shock pressure.
Co-Al porous materials were fabricated by thermal explosion (TE) reactions from Co and Al powders in a 1:1 ratio using NaCl as a space retainer. The effects of the NaCl content on the temperature profiles, phase structure, volume change, density, pore distribution and antioxidation behavior were investigated. The results showed that the sintered product of Co and Al powders was solely Co-Al intermetallic, while the final product was Co4Al13 with an abundant Co phase and minor Co2Al5 and Co-Al phases after added NaCl dissolved out, due to the high Tig and low Tc. The open porosity of sintered Co-Al compound was sensibly improved to 79.5% after 80 wt.% of the added NaCl dissolved out. Moreover, porous Co-Al intermetallic exhibited an inherited pore structure, including large pores originating from the dissolution of NaCl and small pores in the matrix caused by volume expansion due to TE reaction. The interconnected large and small pores make the open cellular Co-Al intermetallic suitable for broad application prospects in liquid–gas separation and filtration.