The magnetodielectric response of magnetoactive elastomers (MAEs) in its dependence on filler concentration, magnetic field, and test frequency is studied experimentally. MAEs are synthesized on the basis of a silicone matrix filled with spherical carbonyl iron particles characterized by a mean diameter of 4.5 µm. The concentration of the magnetic filler within composite materials is equal to 70, 75, and 80 mass%. The effective lossless permittivity ε′ as well as the dielectric loss tanδ grow significantly when the magnetic field increases. The permittivity increases and the dielectric loss decreases with increasing filler concentration. In the measurement frequency range between 1 kHz and 200 kHz, the frequency hardly affects the values of ε′ and tanδ in the absence of a magnetic field. However, both parameters decrease considerably with the growing frequency in a constant magnetic field. The more strongly the magnetic field is applied, the larger the change in permittivity and loss tangent at the same test frequency is observed. An equivalent circuit formulation qualitatively describes the main tendencies of the magnetodielectric response.
New non-crystallizable low-dispersity star-shaped polydimethylsiloxanes (PDMS) containing stereoregular cis-tetra(organo)(dimethylsiloxy)cyclotetrasiloxanes containing methyl-, tolyl- and phenyl-substituents at silicon atoms and the mixture of four stereoisomers of tetra[phenyl(dimethylsiloxy)]cyclotetrasiloxane as the cores were synthesized. Their thermal and viscous properties were studied. All synthesized compounds were characterized by a complex of physicochemical analysis methods: nuclear magnetic resonance (NMR), FT-IR spectroscopy, gel permeation chromatography (GPC), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), viscometry in solution, rheometry, and Langmuir trough study.
We present a novel type of magnetorheological material that allows one to restructure the magnetic particles inside the finished composite, tuning in situ the viscoelasticity and magnetic response of the material in a wide range using temperature and an applied magnetic field. The polymer medium is an A-g-B bottlebrush graft copolymer with side chains of two types: polydimethylsiloxane and polystyrene. At room temperature, the brush-like architecture provides the tissue mimetic softness and strain stiffening of the elastomeric matrix, which is formed through the aggregation of polystyrene side chains into aggregates that play the role of physical cross-links. The aggregates partially dissociate and the matrix softens at elevated temperatures, allowing for the effective rearrangement of magnetic particles by applying a magnetic field in the desired direction. Magnetoactive thermoplastic elastomers (MATEs) based on A-g-B bottlebrush graft copolymers with different amounts of aggregating side chains filled with different amounts of carbonyl iron microparticles were prepared. The in situ restructuring of magnetic particles in MATEs was shown to significantly alter their viscoelasticity and magnetic response. In particular, the induced anisotropy led to an order-of-magnitude enhancement of the magnetorheological properties of the composites.
In this study, we present experimental investigations of the surface structure and water contact angles of magnetoactive elastomers (MAEs), which are controlled by an external magnetic field. Specifically, we examine how the polymer matrix architecture affects the surface roughness and wettability of MAEs in various magnetic fields. We performed a comparative analysis on MAEs based on a linear polysiloxane network and on a matrix of the same chemical nature containing side-grafted chains. We synthesized a series of magnetoactive elastomers containing 75 wt.% carbonyl iron and varying amounts of a low-molecular-weight plasticizer. Although the magnetorheological effect is higher for traditional linear MAEs, we found that the magnetic response in surface properties is higher for novel MAEs with side-grafted chains. The largest increase in water contact angle was observed in the side-chain MAEs with the highest 60 wt.% plasticizer content: rising from 112° in a zero field to 168° in a 490 mT magnetic field. Water contact angles exhibit greater stability over time for side-chain MAEs, and this stability further increases in the presence of a magnetic field. Our results demonstrate that the architecture of the polymer matrix serves as an effective tool for designing smart, magnetically responsive surfaces.
Two-layered structures consisting of piezopolymer and magnetic elastomer were investigated as magnetoelectric material. Three types of magnetic elastomer based on cobalt ferrite (CoFe2O4) and Ni- or Zn-substituted CoFe2O4 nanoparticles were used as magnetically sensitive layers. Cobalt ferrite nanoparticles are considered one of the most promising metal-oxide nanomaterials because of their favorable magnetic properties, such as high saturation magnetization and magnetic anisotropy. The substitution of Co2+ in cobalt ferrite with other transition metals allows for additional tailoring of these properties. The modified magnetic behavior of the substituted CoFe2O4 nanoparticles directly influenced the magnetic properties of magnetic elastomers and, consequently, the magnetoelectric response of composite structures. In this case, the resonant frequency of the magnetoelectric effect remained largely independent of the type of magnetic nanoparticles in the magnetic elastomer layer but its magnitude increased upon Zn substitution up to ~107 mV·cm−1·Oe−1. These findings highlight the potential of chemically engineered magnetic properties of CoFe2O4 nanoparticles for manufacturing magnetoelectric composites to expand their applications in energy harvesting and sensors.
1 December 2024 in Moscow University Physics Bulletin