Lyudmila Galkova

Dr. Lyudmila Galkova

orcid

Research Focus & Metrics

Academic Career Length

18Years (2009-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
11 November 2019 in International Journal of Minerals, Metallurgy and Materials
Verified
Journal Article
Closed access
PDF file
ESEvgeniy Nikolaevich Selivanov
Evgeniy Nikolaevich Selivanov
KPKirill Pikulin
Kirill Pikulin
LGLyudmila Galkova
Lyudmila Galkova
RGRoza Gulyaeva
Roza Gulyaeva
SPSofya Petrova
Sofya Petrova

1 February 2009 in Russian Journal of Non-Ferrous Metals
Verified
Journal Article
Closed access
PDF file
SSS. V. Skopov
S. V. Skopov
SNS. S. Naboichenko
S. S. Naboichenko
LGLyudmila Galkova
Lyudmila Galkova
During the electrosynthesis of manganese dioxide, the anode material and anode current density (i a) exert the largest influence on the characteristics of electrolysis and the quality of the obtained material. The activation of anodes, which consists of the deposition of the titanium-manganese alloy on the titanium base of the electrode by the thermal-diffusion method, prevents passivation at i a = 100 and 200 A/m2. The electrochemical characteristics of electrolysis for NTMA (a built-up titanium-manganese activated anode) and ATDP (an experimental activated anode with thermodiffusion coating) anodes at i a = 100 and 200 A/m2 have close values. The voltage across the bath does not exceed 2.2–3.0 V, the current efficiency is 95–98%, and electrical power consumption is 1.33–1.80 (kW h)/kg. The chemical composition and the crystalline modification of electrical manganese dioxide corresponds to the requirements of GOST (State Standard) 25823-83. The activated ATDP anodes behave similarly to the known HTMA anodes. After electrolysis, no variations in the surface layer are found on them.

10 May 2021 in Metallurgist
Verified
Journal Article
Closed access
PDF file
ESE. N. Selivanov
E. N. Selivanov
DND. O. Novikov
D. O. Novikov
LGLyudmila Galkova
Lyudmila Galkova

30 November 2017 in Tsvetnye Metally
Verified
Journal Article
Closed access
KPKirill Pikulin
Kirill Pikulin
ESE. N. Selivanov
E. N. Selivanov
LGLyudmila Galkova
Lyudmila Galkova
RGR. I. Gulyaeva
R. I. Gulyaeva
We substantiated the treatment regimes for spent catalysts to obtain calcium tungstate. The technology, which allows to obtain calcium tungstate from low-quality raw materials, was taken as a basis. It provides for oxidative roasting, cinder sintering with soda, water leaching of sintered mass and precipitation of calcium tungstate from solution. The spent hydrotreating catalyst was taken as an initial sample. The composition of the catalyst is as follows, %: 13.7 W, 2.7 Ni, 28.2 Al, 7.8 S, 0.3 Si, 2.6 Fe and 20.0 C. According to X-ray phase analysis, the main phase of the catalyst is γ-Al2O3. Tungsten, nickel and iron are represented as oxides (WO3, NiO, Fe2O3), sulfides (WS2, NiS, FeS) and NiWO4 compounds. High content of carbon complicates the hydrometallurgical processing of catalyst. And high sulfur content does not allow its use for direct alloying of steel. Oxidative firing of the catalyst was used to reduce the carbon and sulfur contents. According to the data of thermal and X-ray diffraction (XRD) analyzes, the features of phase formation during oxidative roasting (900 оC) of spent catalysts were established. The process was accompanied by oxidation of carbon and sulfides and the formation of oxides of tungsten, nickel, iron and Al2(WO4)3. The formation of Al2(WO4)3 prevented the complete extraction of tungsten in the solution during leaching. The transfer of tungsten into a water-soluble form is possible by sintering the calcined catalyst with sodium carbonate at a temperature of 800 оC. According to the XRF data, the basis of the sintered mass was sodium tungstate. Oxides of aluminum, iron and nickel were also identified. After aqueous (90–100 оC) leaching (l : s = 4), the oxides of aluminum, nickel and iron were concentrated in the cake. Calcium tungstate was precipitated from the solution by calcium nitrate at a pH of 10–12 and a temperature of 90–95 оC. It contained, %: 58.9 W, 13.9 Ca, 0.37 S. The extraction of tungsten in a commercial product was close to 90%.

4 May 2020 in Materials Science Forum
Verified
Journal Article
Closed access
PDF file
ESE.N. Selivanov
E.N. Selivanov
KPKirill Pikulin
Kirill Pikulin
RGR.I. Gulyaeva
R.I. Gulyaeva
LGLyudmila Galkova
Lyudmila Galkova
The kinetics and mechanism of the natural wolframite interaction with sodium and potassium carbonate, when they are heated in the air, are studied. Using X-ray phase and X-ray structure microanalysis, it was established that the initial single crystal wolfram consists of Fe0.5Mn0.5WO4 and Fe0.3Mn0.7WO4. The method of differential thermal and subsequent phase analysis of products has shown that the interaction of wolframite with sodium and potassium carbonates begins above 450-470 °C with the formation of tungstate and ferrites of sodium and potassium, iron and manganese oxides. Conducting the model experiments on sintering with the subsequent removal of water-soluble compounds (alkalization) made it possible to follow the change in the structure of wolframite. Unit cells parameters of wolframites in solid products (cakes) of leaching do not change if sintering is carried out in the range up to 600 °С. In samples, the preparation of which is coupled with heating to 700–800 °C, the atomic ratio of Fe/Mn in wolframite decreases to 0.2. This allows to specify the mechanism of the process and judge the greater reactivity of wolframites with an increased proportion of iron. Thermal analysis with data processing using the methods of non-isothermal kinetics has established that the studied interactions proceed according to a two-stage mechanism, which in the first stage is limited by diffusion. The appearance of a low-melting eutectic Na2WO4 – Na2CO3 и K2WO4 – K2CO3 in the system contributes to the process transition to the autocatalytic mode.

6 October 2024 in Applied Sciences
Verified
Journal Article
Open access
PDF file
KPKirill Pikulin
Kirill Pikulin
LGLyudmila Galkova
Lyudmila Galkova
GVGalina Vitkina
Galina Vitkina
Antonina KarlinaAntonina Karlina
Antonina Karlina
The loss of quality of wolframite concentrates determines the need to improve their processing method that ensures maximum conversion of tungsten into water-soluble wolframate and a reduction in water-soluble impurities. The results of thermodynamic modeling of the sintering of wolframite concentrate with sodium and potassium carbonates indicate a greater efficiency of K2CO3: The reagent consumption required for complete conversion of tungsten into solution decreases from 170% from stoichiometric sintering with Na2CO3 to 110% for K2CO3, as well as the proportion of soluble silicates up to 0.1%. In addition, sintering with K2CO3 is accompanied by the formation of compounds with a higher melting point, preventing melting and coating formation during the process. Mathematical sintering models were obtained by the method of probabilistically deterministic planning of this experiment. Optimal parameters have been determined: The extraction of tungsten into a solution of more than 95% is achieved by sintering with K2CO3 in an amount of 105–110% according to the stoichiometric requirements for the formation of K2WO4, K2MoO4, and K2SO4 at temperatures of 1073–1123 K for 100–120 min. Pilot tests have confirmed the effectiveness of the process. The possibility of sintering a cinder of wolframite concentrate with K2CO3 without the introduction of recycled materials has been established. Sintering under optimal conditions ensures the transition of tungsten to water-soluble tungstate by 97.5%.