Naiyan Zhang

Dr. Naiyan Zhang

orcid

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
11 May 2018 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
Verified
Journal Article
Closed access
NZNaiyan Zhang
Naiyan Zhang
DZDezhi Zeng
Dezhi Zeng
ZZZhi Zhang
Zhi Zhang
WZWentao Zhao
Wentao Zhao
GYGuangju Yao
Guangju Yao
The effect of element sulphur on the performance of corrosion inhibitor in H2S/CO2 gas field solution was investigated at different velocities. The morphology and composition of corrosion products were characterised by scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) methods. The results indicated that L360 QS steel surface suffered from sulphur-induced pitting corrosion at a low velocity due to insufficient sulphur-carrying fluid power. At high flow velocities, the steel surface is likely to be suffered high fluid power which can remove the inhibitor film and corrosion scales by the mechanical erosion effect. The sulphur corrosion mechanism model and the flow-induced corrosion model due to the high wall shear force have been proposed in the study. This work suggested that the gas production rate should be controlled at an acceptable level to guarantee the service safety of pipeline system.

1 November 2018 in Journal of Petroleum Science and Engineering
Verified
Journal Article
Closed access
NZNaiyan Zhang
Naiyan Zhang
ZZZhi Zhang
Zhi Zhang
ZRZhenhua Rui
Zhenhua Rui
JLJing Li
Jing Li
CZCheng Zhang
Cheng Zhang
SPShirish Patil
Shirish Patil

28 September 2017 in Materials and Corrosion
Verified
Journal Article
Closed access
PDF file
ZZZhi Zhang
Zhi Zhang
NZNaiyan Zhang
Naiyan Zhang
ZLZhiwei Liu
Zhiwei Liu
WZWentao Zhao
Wentao Zhao

1 July 2019 in Anti-Corrosion Methods and Materials
Verified
Journal Article
Closed access
NZNaiyan Zhang
Naiyan Zhang
DZDezhi Zeng
Dezhi Zeng
Purpose: Bimetallic composite pipe consists of a corrosion resistance alloy (CRA) layer for corrosion resistance and carbon steel for mechanical properties, which shows a promising prospect of gathering pipeline with its effective-cost and reliable corrosion resistance. However, the corrosion resistance of composite pipe is determined by the quality of its welding gap. This paper aims to investigate the TIG welding gap corrosion resistance of X52/825 metallurgical clad pipe in H2S/CO2 environment. Design/methodology/approach: Corrosion tests of X52/825 welding gap were performed in a stimulated gas field solution containing both 1 MPa CO2 and 1.5 MPa H2S at 70°C for 720 h in a self-designed high temperature and high pressure autoclave. The anti-stress corrosion cracking (SCC) performance of X52/825 clad pipe ring root welding gap was investigated in both NACE A solution and the stimulant gas field solution by four point bending testing and constant load test. Then the experiments were rerun in XX high sour gas well. In addition, the alloy diffusion and microstructure characteristics of TIG welding gap were analyzed through scanning electron microscopy and energy dispersive X-ray spectroscopy technologies. Findings: The results reveal that the root welding gap is almost not corroded in the stimulant gas field solution, and no micro-cracks were observed by electron microscope. Anti-SCC test results show the root welding gap does not break, indicating a good resistance to environmental-cracking in H2S/CO2 environment. The transition layer can be obviously observed in the root welding zone, and the alloy content of transition layer is diluted. However, the transition layer does not penetrate into the inner of CRA layer, which illustrates its good anti-corrosion performance. Therefore, TIG welding technology can be well used in the welding process of composite pipe. Originality/value: This paper may provide theoretical reference for manufacturing and application of clad pipe.

21 March 2024
Verified
Book Chapter
Closed access
PDF file
NZNaiyan Zhang
Naiyan Zhang
JYJian Yang
Jian Yang
GTGeng Tang
Geng Tang
LZLin Zhang
Lin Zhang
DZDa-Jiang Zhu
Da-Jiang Zhu

5 November 2025 in Processes
Verified
Journal Article
Open access
PDF file
NZNaiyan Zhang
Naiyan Zhang
YLYufei Li
Yufei Li
GTGeng Tang
Geng Tang
HGHao Gong
Hao Gong
DZDajiang Zhu
Dajiang Zhu
QHQiyao He
Qiyao He
In high-sulfur environments, the failure risk of completion tubing increases due to the coupling effect of mechanical and electrochemical corrosion during the acidification production process. The corrosion behavior of P110SS tubing steel was investigated by an HTHP corrosion weight loss experiment and an electrochemical corrosion experiment. Scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS) were used to analyze the surface morphology of the corrosion products. In addition, a prediction model for the remaining service life of completion tubing under the synergistic effect of corrosion and stress was established during the acidification production process. The results show that acidification operations have a significant impact on the subsequent service life of tubing; the corrosion rate of P110SS tubing in the full acidification production process is much higher than that after the produced gas field solution corrosion treatment alone. Obvious pitting marks, micropores, and microchannels are observed in the corrosion product film of P110SS steel after acidification treatment, and the corrosion product film structure of P110SS steel is loose and honeycomb-like after acidification production treatment. The corrosion products are mainly FexSy and FeCO3 after acidification production corrosion treatment. The corrosion during the acidification production stage is controlled by cathodic polarization. The remaining service life of tubing after production corrosion treatment can reach up to 29 years, while the remaining service life of tubing after acidification production corrosion treatment is significantly reduced, with a maximum of only 8 years. The research results have guiding significance for the selection, optimization, and design of high-sulfur-gas well tubing.