The development of hydrometallurgical recycling processes for lithium-ion batteries is challenged by the heterogeneity of the electrode powders recovered from end-of-life batteries via physical methods. These electrode materials, known as black mass, vary in composition, containing differing amounts of nickel, manganese, and cobalt (NMC), as well as other chemicals, such as lithium iron phosphate (LFP). This study presents the results of the hydrometallurgical treatment of mixed NMC and LFP black masses aimed at creating flexible recycling processes. This approach leverages the reducing power of LFP to optimize the leach liquor composition for re-synthesizing NMC precursors. In particular, the leaching conditions were optimized based on the LFP content in the solid feed to maximize the extraction of key metals (Ni, Mn, Co, and Li). The leaching solid residue, graphite, was treated and characterized as a secondary raw material for new anode preparation. Iron phosphate was recovered by increasing the pH of the leach liquor, and the NMC precursors were obtained via coprecipitation. This process achieved a recycling rate of 51%, based on the black mass input and the mass of recovered elements in the output products. Additionally, substituting LFP scraps as the reducing agent in place of H2O2 reduced the recycling process’s environmental impact by avoiding 1.7 tons of CO2-equivalent emissions per ton of NMC black mass.
The hydrometallurgical recycling of end-of-life Li-ion batteries constitutes a sustainable path for the integral recovery of battery components. However, the heterogeneity of electrode materials constitutes a limitation for process optimization that must provide robust and flexible strategies. In this work, the preliminary results obtained as part of the demonstration activities of the LIFE DRONE project are reported with particular attention to the possibility of integrating the recycling process based on the resynthesis of NMC (Nickel Manganese Cobalt) cathodes with the treatment of mixed black mass also containing LFP (Lithium Ferrous Phosphate) electrodic powders. The experimental results obtained highlight the possibility of leaching NMC black mass in the absence of hydrogen peroxide when NMC-LFP mixtures are used with almost quantitative extraction yields of metals. In particular, working without H2O2 at 60°C for 3 h the following yields of extraction were obtained: 89% for Ni, 69% for Mn, 89% for Co, 91% for Li, 90% for Fe, 100% for P, 56% for Al and 32% for Cu. Furthermore, the experimental data showed that by varying the pH of the leach liquor, it is possible to separate selectively iron phosphate by quantitative precipitation (100% for Fe, 100% for P and 60% for Al) before proceeding with NMC resynthesis.