As a main apparatus, the oxygen lance is used to deliver the oxygen element and transfer kinetic energy into the molten bath in the steelmaking process. However, the Laval nozzle exit would be gradually worn out during the service life, which suppresses the performance of the oxygen lance. This paper investigated three different wear length (Lw) conditions at the exit of the Laval nozzle through numerical simulations and high-temperature experiments with various oxygen flow rates. The result showed that the entrainment of the ambient gas was the key factor of the wear phenomenon for the Laval nozzle exit. The maximum total temperature of the gas phase at the Laval nozzle exit formed by the Lw of 0 mm, 2 mm, and 4 mm were 300 K, 959 K, and 1700 K, respectively. Thus, by increasing the Lw value, the total temperature of the gas phase was rapidly improved at the exit of the Laval nozzle, which further accelerated the wear phenomenon at the exit of the Laval nozzle. Besides, axial velocities at the end of the potential core formed by the Lw of 0 mm, 2 mm, and 4 mm were 483.7 m/s, 480.0 m/s, and 478.7 m/s, respectively. As a result, the wear phenomenon reduced the impaction ability of the oxygen jet, which suppressed the impaction depth and radius, resulting in a smaller droplet generation rate.
To reduce the production costs of ultra-low carbon steel, an oxygen lance has been employed in a 150 t decarburization ladle furnace. This study conducted both water experiments and numerical simulations to examine the flow field characteristics and stirring effects of the top-blowing lance at various inclination angles of 4°, 6°, 8°, and 10°. The results indicated that a smaller inclination angle enhanced the mixing effect and impaction depth of the molten bath, whereas the impaction diameter exhibited a contrasting trend. The behavior of the oxygen multi-jets suggested that a smaller inclination angle mitigated the loss of kinetic energy, thereby improving impaction ability. As the depth of the molten bath increased, the average velocity of the molten bath section displayed a trend characterized by an initial rapid decrease, followed by a gradual decline, and culminating in a subsequent rapid drop. In industrial application research, the 4° oxygen lance resulted in a shorter decarburization time compared to the 8° oxygen lance. This reduction in decarburization time led to decreased heat energy loss due to the heat-absorbing effect of ambient gas, which further enhanced the end-point temperature of the molten bath.