As a main apparatus, the oxygen lance is used to deliver the oxygen element and transfer kinetic energy into the molten bath in the steelmaking process. However, the Laval nozzle exit would be gradually worn out during the service life, which suppresses the performance of the oxygen lance. This paper investigated three different wear length (Lw) conditions at the exit of the Laval nozzle through numerical simulations and high-temperature experiments with various oxygen flow rates. The result showed that the entrainment of the ambient gas was the key factor of the wear phenomenon for the Laval nozzle exit. The maximum total temperature of the gas phase at the Laval nozzle exit formed by the Lw of 0 mm, 2 mm, and 4 mm were 300 K, 959 K, and 1700 K, respectively. Thus, by increasing the Lw value, the total temperature of the gas phase was rapidly improved at the exit of the Laval nozzle, which further accelerated the wear phenomenon at the exit of the Laval nozzle. Besides, axial velocities at the end of the potential core formed by the Lw of 0 mm, 2 mm, and 4 mm were 483.7 m/s, 480.0 m/s, and 478.7 m/s, respectively. As a result, the wear phenomenon reduced the impaction ability of the oxygen jet, which suppressed the impaction depth and radius, resulting in a smaller droplet generation rate.
The copper was the main manufacturing material to produce the coherent lance for enhancing the cooling effect. Due to the low hardness of copper and high-temperature environment, the exit of Laval nozzle would be worn off, resulting in suppressing the impaction ability of supersonic oxygen jet. In order to investigate the effect of wear length on the behavior of coherent jet, both high-temperature experiment and numerical simulation have been carried out, and the axial velocity, total temperature and oxygen fraction were measured in the experimental test to verify the accuracy of simulation model. Based on the result, the overexpand phenomenon was generated due to the Laval nozzle exit wear off, which improved the shock wave intensity at the tip of Laval nozzle, resulting in a lower axial velocity at the velocity potential core. With a longer wear length, the vorticity of the coherent jet periphery is increased, which causes more thermal energy of combustion flame being released prematurely near the coherent lance tip, leading to a shorter velocity potential core.
Utilizing the greater momentum inertia and higher specific surface area of powder lime, top-blown CaO-O2 technology has been proposed to further improve the mixing ability of the molten bath and to increase the slagging rate in the Basic Oxygen Furnace (BOF) steelmaking process. This research presented the development of a simulation model designed for investigating the effect of centre CaO-O2 mixed injection method on the flow field within the molten bath. The result showed that, compared to the traditional jet, the CaO-O₂ jet improved axial impaction ability of top-blown jet, while reducing its impaction ability in the radial direction. Furthermore, the CaO-O₂ jet not only improved the impaction depth, but also exhibited a smaller decrease rate in impaction depth as the lance height increased. In the conical protrusion area, a greater amount of kinetic energy from the CaO-O₂ jet was transferred into the molten bath, which enhanced the dynamic condition within the molten bath.
1 April 2024 in Metallurgical and Materials Transactions B
In order to suppress the rapid combustion effect and consumption rate of pure hydrogen gas, N2 or CO2 at flow rates of 0, 80, and 240 Nm3/h was pre-mixed with shrouding H2 at flow rates of 800, 720, and 560 Nm3/h at room temperature, and the behaviors of the main oxygen jet and shrouding flame were analyzed by both numerical simulation and combustion experiments. The results showed that, because of the participation of CO2 in the H2 combustion reaction, the length of the axial velocity potential core was reduced using the CO2 shrouding mixed injection method, compared to the same mixed rate of N2. This trend would be further enhanced as N2 and CO2 mixing ratio increased. Meanwhile, when the shrouding mixed rate is 30%, the maximum axial and radial expansion rate generated by N2-H2 shrouding method is 1.28 and 1.04 times longer than that by the CO2-H2 shrouding method. The Fo-a, theoretical impaction depth and area generated by the 10% N2 shrouding mixed rate was 84.0, 95.5 and 86.4% of those generated by the traditional coherent jet, respectively, which indicated that the 10% N2 shrouding mixed rate method might lead to comparable production indexes in the EAF steelmaking process.