The corrosion behavior of soluble Mg–Gd-based alloys was systematically investigated by analyzing two key aspects: environmental factors and microstructural characteristics. Environmental influences were evaluated using immersion weight loss tests under varying Cl− concentrations and temperature conditions. From a microstructural perspective, the study examined the impact of different initial microstructural morphologies on corrosion performance. The second-phase compound Mg5Gd, formed in alloys prepared via melting, was subjected to both immersion weight loss and electrochemical testing. The results demonstrated that corrosion rates increased with higher Cl− concentrations and elevated temperatures, albeit in a nonlinear manner. Notably, significant effects on corrosion rates were observed in the Cl−concentration range of 1% to 3% and at temperatures between 75 °C and 100 °C. Additionally, the dissolution rate of the alloy increased markedly from 8.37 mg/cm2/h in the as-cast state to 43.85 mg/cm2/h following extrusion combined with perforation deformation. Microstructural analysis revealed that the extrusion process disrupted the coarse, reticulated second-phase structure observed in the as-cast state, thereby diminishing its corrosion-inhibiting properties. Electrochemical testing further confirmed that the Mg5Gd second phase, formed through the incorporation of the rare-earth element Gd, exhibited high electrochemical activity.
In this study, the high-temperature thermal deformation behavior of the TA4 alloy was investigated by thermal compression experiments. The effects of deformation temperature and strain rate on the rheological stress are described by analyzing the variation of stress–strain curves with different parameters and establishing the constitutive equation based on the dynamic material theory model. Thermal processing diagrams were established and plotted to analyze the optimal processing zone and the destabilization zone under different strains. From the thermal machining diagram, it can be concluded that the optimum machining zone at a strain of 0.9 is 1040~1133 K/0.01~0.7 s−1. The optimum machining zone at a strain of 0.6 is 940~1000 K/0.01~0.04 s−1. The optimum machining zone at a strain of 0.3 is 940~1000 K/0.01~0.08 s−1. The effects of different deformation conditions on the thermal deformation mechanism were analyzed in conjunction with EBSD characterization. The results showed that dynamic recrystallization (DRX) was the main deformation softening mechanism when at low strain rate (≤0.1 s−1). At higher strain rates (>0.1 s−1) and lower temperatures (<1083 K and ≥933 K), the main deformation softening mechanism was DRV; at higher temperatures (≥1083 K and ≤1133 K), the main deformation softening mechanism was DRX.
To address the problems of coarse grains and unsatisfactory mechanical properties of as-cast Mg-8.5Al-1Zn alloy, which hinder its application in dissolvable bridge plugs, this study took the alloy as the research object and subjected it to plastic deformation via hot extrusion with an extrusion ratio of 12. Through the use of Combined Electron Backscatter Diffraction (EBSD) and Transmission Electron Microscopy (TEM) Testing and Characterization Techniques, the macroscopic mechanical properties, microstructural evolution, and extrusion deformation mechanism of the alloy in both as-cast and as-extruded states were systematically investigated. The results indicate that hot extrusion deformation significantly enhances the comprehensive mechanical properties of the alloy. Compared with the as-cast alloy, the tensile strength, yield strength, and elongation of the as-extruded alloy are increased by 104.0%, 314.9%, and 166.7%, respectively, with the static toughness increasing by 809.1%. The as-cast alloy exhibits coarse grains, Al element segregation, and high-density dislocations. After hot extrusion, dynamic recrystallization dominates the grain refinement, reducing the grain size by approximately 60%. Solute atoms precipitate to form multiphase structures and coherent nano-scale precipitates, along with the formation of tensile twins and a weakened bimodal texture. The improved yield strength of the as-extruded alloy stems from the synergistic effect of multiple strengthening mechanisms, among which precipitation strengthening induced by nano-precipitates is the primary contributor. The enhanced plasticity is attributed to grain refinement and texture regulation. This study clarifies the extrusion deformation mechanism of the Mg-8.5Al-1Zn alloy for dissolvable bridge plugs and verifies the rationality of the hot extrusion process with an extrusion ratio of 12, providing technical support for its industrial application in dissolvable bridge plugs and the performance regulation of similar dissolvable magnesium alloys.
In order to investigate the corrosion behavior of Mg-Gd based soluble magnesium alloy materials, two aspects, environmental factors and microstructural point of view, were discussed in this study respectively. Among them, the environmental factor aspect was carried out by immersion weight loss tests at different Cl- concentrations and different temperatures. In terms of microstructure, the influence of different initial tissue morphologies on the corrosion behavior of the alloy was mainly investigated, and the second phase Mg5Gd, prepared by melting, was subjected to immersion weight loss tests and electrochemical tests. The results show that the corrosion rate of the alloy increases with the increase of Cl- concentration and temperature, but the growth trend is not linear, in which the Cl- concentration of 1% to 3% and the temperature of 75 °C to 100 °C have a significant effect on the corrosion rate of the alloy, respectively; the dissolution rate of Mg-Gd-based soluble magnesium alloy after extrusion + perforation deformation was greatly improved from 8.37 mg/cm2/h in the as-cast state to 43.85 mg/cm2/h. Combined with the microstructure analysis, it is believed that the extrusion destroys the coarse reticulated second phase in the as-cast state organization, which reduces the corrosion-blocking network effect of the second phase; electrochemical tests showed that the second phase Mg5Gd formed after the addition of the rare earth element Gd had a high electrochemical activity.
In this study, the high-temperature thermal deformation behavior of TA4 alloy was investigated through thermal compression experiments. The effects of deformation temperature and strain rate on rheological stress were analyzed by examining the variations in stress-strain curves under different conditions and establishing a constitutive equation based on the dynamic material theory model. The prediction accuracy of the developed constitutive model was evaluated, yielding a correlation coefficient of 0.9612 between predicted and experimental values, an average absolute percentage error of 8.7210%, and an average root mean square error of 11.0635 MPa. Thermal processing diagrams were established and plotted to analyze the optimal processing zone and the destabilization zone under different strains. The optimal processing zones at different strains are obtained from the thermal processing diagrams, which are 1040~1133K, 0.01~0.7s-1 at a strain of 0.9, 940~1000K, 0.01~0.04 s-1 at a strain of 0.6, 940~1000K, 0.01~0.08s-1 at a strain of 0.3, 940~1000K, 0.01~0.08s-1 at a strain of 0.3. Additionally, the thermal deformation mechanisms of TA4 alloy under varying deformation parameters were analyzed using EBSD characterization. The results indicate that the primary deformation softening mechanisms include dynamic recovery (DRV) at low temperatures and high strain rates, dynamic recrystallization (DRX) at high temperatures and high strain rates, and DRX at low strain rates.