In a way so far unmatched in any single study, this paper presents the complex characteristics of commercially pure titanium (CP-Ti) containing 0.2 wt.% carbon, which is significantly above the carbon level in commonly used titanium alloys, while at the same time being the maximum permitted content in light of the recommendations in force. It has been demonstrated that the addition of carbon in CP-Ti can have many positive impacts. The investigated Ti-0.2C alloy was produced in a cold-copper crucible induction vacuum furnace and processed into a 12 mm diameter bar by hot rolling. The structure and properties of the Ti-0.2C alloy were compared to those of an CP-Ti Grade 1 produced and processed under the same technical conditions. The addition of 0.2 wt.% carbon to CP-Ti has been found to change the course of the crystallization process, the course and temperatures of phase transformations, and the values of lattice parameters; reduce susceptibility to grain growth; and create the possibility for additional hardening during solution treatment and aging. At the same time, it results in an assumed improvement in properties by increasing the tensile strength and yield strength, hardness, creep and oxidation resistance, and abrasive wear. It has a negative effect but is still within the acceptable range on impact strength and susceptibility to hot and cold deformation.
This paper presents the chemical and phase composition, microstructure, and selected properties both at room temperature and at the temperature corresponding to the expected operating conditions of three successive generations of TiAl-based alloys (Ti-47Al-2W-0.5Si, Ti-45Al-8Nb-0.5(B,C), and Ti-45Al-5Nb-2Cr-1Mo-0.5(B,C)-0.2Si) melted in a vacuum induction furnace with high-density isostatic pressed graphite crucibles. The obtained results of mechanical and physical properties of the produced alloys were compared to the properties of reference alloys with similar chemical composition and melted in a cold copper crucible furnace. The effect of increased carbon content in the produced alloys due to the degradation of the graphite crucible during melting is higher strength properties, lower plastic properties, higher coefficient of thermal expansion, and improved creep resistance. It was shown that the proposed technology could be successfully used in the production of different generation TiAl-based intermetallic alloys.
13 December 2017 in Materials Science and Technology
In the paper, the phase composition, microstructure, and selected mechanical and operational properties at room and elevated temperature of a TiAl intermetallic alloy from the TNB group – Ti–45Al–8Nb–0.5(B, C), induction melted in special graphite crucibles, are characterised. Selected properties of this alloy were compared to those of the reference TNB-V2 alloy with similar chemical composition, prepared with technologies currently used in the world. The result of this comparison was a positive recommendation for the proposed melting technology as an alternative to this and other groups of TiAl-based alloys. This paper is part of a thematic issue on Titanium.
1 March 2017 in Archives of Metallurgy and Materials
This paper presents the possibilities of forming the microstructure as well as mechanical properties and electrical conductivity of Cu-3Ti alloy (wt.%) in thermal and thermomechanical processes that are a combination of homogenising treatment, hot and cold working, solution treatment and ageing. Phase composition of the alloy following various stages of processing it into the specified semi-finished product was being determined too. It was demonstrated that the application of cold plastic deformation between solution treatment and ageing could significantly enhance the effect of hardening of the Cu-3Ti alloy without deteriorating its electrical conductivity. It was found that for the investigated alloy the selection of appropriate conditions for homogenising treatment, hot and cold deformation as well as solution treatment and ageing enables to obtain the properties comparable to those of beryllium bronzes.
One of the major barriers limiting the suitability of TiAl intermetallic alloys for use in the demanding aircraft and automotive industries is their susceptibility to degradation as a result of oxidation at temperatures exceeding 760 °C. Paper presents the characteristics of resistance to cyclic oxidation at 950 °C for Ti–45Al–8Nb–0.5(B, C) alloy with and without protective coating obtained as a result of aluminizing using out of pack method. The characteristics of surface condition were determined by scanning electron microscope with EDS system, transmission electron microscope, and X-ray diffractometer. The favorable behavior of the Ti–45Al–8Nb–0.5(B, C) alloy with a protective coating under cyclic oxidation conditions is a result of a higher content of Al2O3 in the microstructure of the scale and the presence of Al and Nb-rich phases at the substrate interface, which probably constitue a barrier for oxidation process. The high temperature oxidation test revealed that aluminide coating was responsible for a remarkable improvement in the oxidation resistance.
This study investigates the characteristics of the Ti-5Al-2.5Sn-0.2C alloy, an alpha titanium alloy containing approximately 0.2 wt% carbon—a concentration significantly exceeding the standard allowable limit of 0.08 wt%. The Ti-5Al-2.5Sn-0.2C alloy was melted in a vacuum induction furnace with a cold copper crucible, processed into bar form through hot rolling, and subsequently annealed under standard conditions. The microstructure and mechanical properties of the Ti-5Al-2.5Sn-0.2C alloy were systematically compared with those of the Ti-5Al-2.5Sn alloy (Grade 6), which possesses a similar chemical composition. The results revealed that the addition of 0.2 wt% carbon significantly influences the alloy’s solidification process, phase transformation temperatures, phase composition, and phase lattice parameters. Moreover, the carbon addition enhances key mechanical properties, including tensile strength, yield strength, hardness, and wear resistance, as well as creep and oxidation resistance. While a slight reduction in plasticity and increase in impact energy were observed, the alloy remained within the permissible range defined by existing standards.