A near-equiatomic FeCoNiCuAl High-entropy alloy (HEA) was produced using laser powder bed fusion (L-PBF) pre-alloy powder. Microstructural characteristics and tribological properties of L-PBF specimens under various volumetric energy densities (VEDs) were investigated in detail. The results showed that the phase of L-PBF specimen consisted of BCC matrix + Cu-rich B2 precipitate. The microstructure of L-PBF specimen largely consisted of columnar grains perpendicular to the melt pool boundary (MPB) direction owing to the epitaxial growth along the temperature gradient. The preferred orientation of the L-PBF specimen was gradually transformed from the order of to as the VED rose. Larger size precipitates re-appeared and wider MPB were formed upon faster remelting and steeper cooling as a result of higher VED. Compared to the components produced by Spark Plasma Sintering, L-PBF specimens presented better wear resistance owing to the ultra-fine substructure and nano-scaled precipitates. In addition, the L-PBF specimen produced with 83 J/mm3VED exhibits the highest elastic strain to failure (H/Er) and yield stress (H2/Er3).
AISI 316L, Ti2, and Zr1 are widely used in the selection of reaction still material, however, there is corrosion wear behavior in the use process. In this paper, the adsorption behavior of oxygen in Fe, Ti, and Zr is studied by the first principles method. Corrosion and wear behaviors of AISI 316L, Ti2 and Zr1 were studied by electrochemical corrosion and wear tests. The results show that AISI 316L can effectively resist the action of friction pair during wear by elastic modulus calculation. Oxygen is easily adsorbed at the top of the Fe(111) crystal plane and the bridge site of the Zr(110) crystal plane to form the most stable adsorption structure. The Ecorr of Zr1 (0.275 V) is greater than that of Ti2 (0.266 V) and AISI 316L (0.094 V), resulting in a ZrO2 passivated film with strong protection in the HNO3 solution. The wear rate of AISI 316L is higher than that of Zr1 and Ti2. In the selection of tin chemical reactor material, it is preferred that Zr1 can withstand corrosion and wear for a long time in a nitric acid system, which provides important guidance for corrosion and wear of reactor materials in the synthesis of tin acid.
The effect of the distribution of the primary phase Si and TiB2 particles in the hypereutectic Al-Si alloy was studied and found to be influenced by the cooling rate. Therefore, this article studies the effect of the cooling rate on the multi-phase structure of TiB2 particles in Al-20Si using a wedge-shaped mold. The sizes, shapes, and distribution of primary phase Si and TiB2 particles inside primary phase Si were observed through SEM. The effect of TiB2 particles on cracks in primary phase Si was studied using nanoindentation technology, and the interface relationship between primary Si and TiB2 was studied using TEM. Finally, based on the experimental results, the trapping mechanism of primary Si for TiB2 particles is discussed. The results indicate that the faster the cooling rate, the finer and more uniform the size distribution of the primary Si phase in the structure. TiB2 mostly exists as individual particles. Moreover, the pushing rate of the solid–liquid interface during solidification is faster, resulting in more TiB2 particles being engulfed by the primary Si phase.