Precision dicing with diamond wheels is a key technology in semiconductor dicing, integrated circuit manufacturing, aerospace, and other fields, owing to its high precision, high efficiency, and broad material applicability. As a critical processing stage, a comprehensive analysis of dicing technologies is essential for improving the machining quality of hard-and-brittle optoelectronic materials. This paper reviews the core principles of precision diamond wheel dicing, including dicing processes and blade preparation methods. Specifically, it examines the dicing mechanisms of composite and multi-mode dicing processes, demonstrating their efficacy in reducing defects inherent to single-mode approaches. The review also examines diverse preparation methods for dicing blades, such as metal binder sintering and roll forming. Furthermore, the roles of machine vision and servo control systems are detailed, illustrating how advanced algorithms facilitate precise feature recognition and scribe line control. A systematic analysis of key components in grinding wheel dicer is also conducted to reduce dicing deviation. Additionally, the review introduces models for tool wear detection and discusses material removal mechanisms. The influence of critical process parameters—such as spindle speed, feed rate, and dicing depth—on dicing quality and kerf width is also analyzed. Finally, the paper outlines future prospects and provides recommendations for advancing key technologies in precision dicing, offering a valuable reference for subsequent research.
To investigate how the process parameters of ultra-thin diamond grinding wheel dicing affect the dicing quality of silicon carbide (SiC) wafers, single-factor experiments were designed. This study examined the influence of key process parameters, including spindle speed, feed rate, and first dicing depth, on the maximum chip width on the front side W1 and the maximum chip width on the back side W2, thereby determining their optimal parameter ranges. Subsequently, a quadratic polynomial prediction model was established using response surface analysis to analyze the interactive effects among the grinding wheel dicing process parameters. Finally, the prediction model was optimized using the genetic algorithm NSGA-II, and the optimal parameter combination for the two response variables was determined: a spindle speed of 31,960 r/min, a feed rate of 2.0019 mm/s, and a first dicing depth of 197.51 μm, yielding an average W1 of 4.8852 μm and W2 of 18.5360 μm. The relative errors between the predicted and average experimental values are 2.83% for W1 and 4.43% for W2. Both errors are below 5%, confirming the validity of the model. Therefore, the model serves as a practical reference for planning subsequent dicing processes using ultra-thin diamond grinding wheels.
Al-50 wt% Si alloy is widely used in aerospace and electronics but is hard to machine owing to uneven microstructure. To elucidate the relationship between force–thermal coupling effects and surface integrity during Al-50 wt% Si alloy milling, this paper established a stress model to reveal the superposition mechanism of mechanical and thermal stresses. Experiments were conducted to investigate the evolution of cutting forces and temperatures, as well as their influence on surface integrity characteristics, including microhardness, roughness, and chip morphology. The results showed that temperature increases steadily with vc, whereas cutting force fluctuates in an irregular manner. The maximum cutting temperature rises by 85.04% as vc increases from 25 m/min to 125 m/min. Meanwhile, the thermo-mechanical coupling effect exerts a regulatory role on chip morphology, where higher vc improves chip continuity and ductility. Surface integrity is determined by the competitive interplay between work hardening and thermal softening, and the surface microhardness varies from 168.49 HV to 173.27 HV. Specifically, elevated vc optimizes surface quality, with the Ra decreasing by 24.54%, whereas excessive fz and ap aggravate damage. Ultimately, surface defects arise from the combined removal behavior of Si particles and deformation of the Al matrix, while the inhomogeneous stress field induces subsurface damage.