The production and quality of automotive-grade galvanised steel are affected by the limited service life of the pot roll bearings used in continuous galvanising lines. The journal bearings are subjected to severe degradation as they react with the molten Zn bath, and coatings can provide corrosion protection to the bearing materials. This research investigates the performance of Al2O3 coatings applied via the HVOF thermal spray process to stainless steel 316L substrates. Immersion tests were conducted in baths of different compositions, namely GI (Zn-0.3 wt.% Al) and ZMA (Zn-1.5 wt.% Al-1.5 wt.% Mg). Material characterisation after testing showed evidence of coating degradation after 1 week, as the coating tended to crack and detach from the substrate, allowing the molten Zn to attack the underlying steel. The coefficient of thermal expansion of Al2O3 and steel was measured, and a difference of 13 × 10−6 K−1 was found, leading to the development of cracks in the coatings. Zn penetration through cracks was determined to be the main failure mechanism of the Al2O3 coatings, which otherwise remained inert to Zn-Al. Conversely, the coatings immersed in Zn-Al-Mg reacted with the Mg in the molten metal bath, showing that changing bath composition affected the performance of the coatings in molten Zn alloy.
Galvanising pot roll bearings are subjected to severe deterioration due to the corrosion of the bearing materials in liquid Zn, resulting in maintenance stops that can cost thousands of pounds per hour in downtime. Dynamic wear testing in molten Zn-Al and Zn-Al-Mg was conducted to assess the corrosion and wear resistance of three material pairs using a bespoke testing rig. The materials investigated in this study were Wallex6TM coated with WC-Co, stainless steel 316L coated with Al2O3, and as-received Wallex6TM and Wallex4TM alloys. It was found that only the Al2O3 coating remained unreactive in Zn alloy, whereas the materials containing Co were corroded, as evidenced by the formation of intermetallic compounds containing Al-Co-Zn-Fe. The results also highlighted that the dissolution of the Co matrix and diffusion of Zn and Al from the bath occurred in Wallex6TM and Wallex4TM. However, the diffusion of Zn into the WallexTM alloys was reduced by approximately 60% in the Zn-Al-Mg bath compared to Zn-Al. The wear scars were analysed to determine the wear coefficient of the worn specimens. Out of the three material couplings investigated in this study, minimal wear damage in both Zn-Al and Zn-Al-Mg was only obtained by pairing Wallex6TM with Al2O3 coatings.