Objectives: To analyze survival and complication rates for anterior and premolar laminate‐veneers out of different ceramic materials (feldspathic, leucite‐reinforced glass–ceramic [LRGC], lithium‐disilicate [LDS] and zirconia).Material and Methods: A systematic literature search was conducted across multiple databases for clinical studies on ceramic laminate‐veneers with a minimum‐follow‐up of ≥ 1 year. The date of last search was on February 19, 2024. Survival, technical, esthetic and biological events were assessed for different laminate‐veneer materials at three observation periods (short‐ [1–3 years], mid‐ [4–6 years] and long‐term [≥ 7 years]).Results: Twenty‐nine studies were included. Meta‐analysis revealed a pooled survival‐rate of 96.13% for feldspathic, 93.70% for LRGC and 96.81% for LDS at 10.4 years. No difference was found between materials. Complication rates (technical/esthetic/biological) were as follows: Feldspathic: 41.48%/19.64%/6.51%; LRGC: 29.87%/17.89%/4.4%; LDS: 6.1%/1.9%/0.45% at 10.4 years. Zirconia showed a 100% survival‐rate with no complications at 2.6 years. No long‐term data was available for zirconia.Conclusions: Feldspathic, LRGC and LDS laminate‐veneers showed high survival‐rates at long‐term observation. LDS slightly outperforms feldspathic and LRGC laminate‐veneers with lower long‐term complication rates. More studies providing long‐term data on zirconia laminate‐veneers are needed.Clinical Significance: Ceramic laminate‐veneers are a reliable treatment option. LDS may be preferred as a restorative material for long‐term success.
1 January 2021 in The Journal of Advanced Prosthodontics
Objective: To analyze the influence of restoration design (partial‐coverage restoration vs. crown) and ceramic layer thickness on the performance and failure loads of CAD/CAM‐fabricated lithium disilicate (LDS) reconstructions on molars after fatigue.Materials and Methods: Seventy‐two posterior monolithic CAD/CAM‐fabricated LDS restorations (IPS e.max CAD, Ivoclar Vivadent) with different occlusal/buccal ceramic layer thicknesses (1.5/0.8, 1.0/0.6, and 0.5/0.4 mm) and restoration designs (PCR: non‐retentive full‐veneer/partial‐coverage restoration, C: crown,) were investigated and divided into six groups (n = 12, test: PCR‐1.5, PCR‐1.0, PCR‐0.5; control: C‐1.5, C‐1.0, C‐0.5). LDS restorations were adhesively bonded (Variolink Esthetic DC, Ivoclar Vivadent) to dentin‐analogue composite dies (Z100, 3M ESPE). All specimens were subjected to thermomechanical loading (1.2 million cycles, 49 N, 1.6 Hz, 5–55°C) and exposed to single load to failure testing. Failure analysis was performed with light and scanning electron microscopies. Data were statistically analyzed using ANOVA, Tukey‐Test, and t‐test (p < 0.05).Results: Eight crown samples (C‐0.5) and one PCR specimen (PCR‐0.5) revealed cracks after fatigue, resulting in an overall success rate of 87.5% (crowns: 75%, PCRs: 96.88%). Direct comparisons of PCRs versus crowns for thicknesses of 0.5 mm (p < 0.001) and 1.0 mm (p = 0.004) were significant and in favor of PCRs. Minimally invasive PCRs (0.5 and 1.0 mm) outperformed crowns with the identical ceramic thickness. No difference was detected (p = 0.276) between thickness 1.5 mm PCRs and crowns.Conclusions: Minimally invasive monolithic CAD/CAM‐fabricated posterior LDS PCRs (0.5 and 1.0 mm) resulted in superior failure load values compared to minimally invasive crowns. Minimally invasive crowns (0.5 mm) are prone to cracks after fatigue.Clinical Significance: Minimally invasive CAD/CAM‐fabricated LDS PCR restorations with a non‐retentive preparation design should be considered over single crowns for molar rehabilitation.
19 November 2024 in Journal of Esthetic and Restorative Dentistry
Objective: To determine the clinical performance of partial coverage restorations (PCR) (onlays, occlusal veneers, and partial crowns) composed of different ceramic and ceramic‐based materials to treat extended posterior defects.Materials and Methods: MEDLINE, Scopus, CENTRAL, ClinicalTrials.gov, and the International Clinical Trials Registry Platform were searched (inception‐February 2024) for randomized controlled trials (RCT) comparing posterior PCRs composed of different ceramic and ceramic‐based materials with a minimum follow‐up of 1 year.Results: Six RCTs were included. Resin matrix ceramic (RMC) and lithium disilicate (LDS) restorations had a 3‐year survival rate of 89.3% (95% CI 76.4–95.3) and 93.7% (95% CI 83.7–97.7), respectively, and leucite‐reinforced glass ceramic (LRGC) restorations a range between 96.1% (95% CI 90.1–98.9) compared with RMC and 98.3% (95% CI 90.8–100) compared with LDS. After 1–3 years of follow‐up, LDS slightly outperformed RMC on restoration failure and loss of retention (1.56 more failures and 1.78 more loss of retentions for RMC per 100 restoration‐years [low certainty evidence]). No statistically significant differences between ceramic and ceramic‐based materials were detected in short‐term follow‐up (1–3 years of follow‐up). The long‐term performance of posterior PCRs is uncertain.Conclusion: The survival of LDS restorations may slightly outperform RMC restorations after 3 years of follow‐up across outcomes, except for bulk fracture. RCTs providing medium to long‐term data are needed.Clinical Significance: Ceramic and ceramic‐based PCRs are a reliable treatment option to restore extended posterior defects.
21 May 2025 in The Journal of Prosthetic Dentistry
Photogrammetry (PG) has emerged as a promising recording technique for fabricating implant-supported prostheses. However, the existing evidence on the accuracy of dental PG devices is still limited. The purpose of this in vitro study was to evaluate the trueness and precision of a newly introduced advanced PG device (MicronMapper; SIN 360) by comparing it with grammetry and intraoral scanning. Four implants (BioHorizons) were placed in an edentulous mandibular model. Multi-unit abutments (BioHorizons) were positioned and tightened to 30 Ncm. A digital reference cast (Control group) was obtained by scanning the model with a laboratory scanner (inEosX5; Dentsply Sirona). Three test groups were evaluated: PS (Primescan), PS-OS (Primescan and OptiSplint), and PG (MicronMapper; SIN 360). Test files were superimposed with the reference file (trueness) and pairwise within groups (precision) using a 3D evaluation software program (Geomagic Control X). Root mean square (RMS) values were calculated. Analysis of variance (ANOVA) was used to analyze differences in RMS values among groups (α=.05), followed by the Tukey post hoc test. For trueness, group PG showed the lowest mean ±standard deviation RMS values (20.5 ±0.6 µm), followed by PS-OS (30.9 ±16.8 µm) and PS (56 ±0.7 µm). A statistically significant difference was found between groups PG and PS (P<.001), as well as PS-OS and PS (P=.004). For precision, the lowest RMS values were detected in group PG (6 ±1.2 µm), followed by PS (9.5 ±3.3 µm) and PS-OS (23.3 ±22.3 µm). No statistically significant differences were detected among the test groups in terms of precision (P=.192). Photogrammetry obtained the best accuracy. Grammetry improves the trueness; however, it appears to have no positive impact on the precision of complete arch implant recordings.
22 August 2023 in Journal of Esthetic and Restorative Dentistry
Objective: To investigate the effect of ceramic thickness and dental substrate (enamel vs. dentin/enamel) on the survival rate and failure load of non‐retentive occlusal veneers.Materials and Methods: Human maxillary molars (n = 60) were divided into five test‐groups (n = 12). The groups (named DE‐1.5, DE‐1.0, DE‐0.5, E‐1.0, E‐0.5) differed in their dental substrate (E = enamel, DE = dentin/enamel) and restoration thickness (standard: 1.5 mm, thin: 1.0 mm, ultrathin: 0.5 mm). All teeth were prepared for non‐retentive monolithic lithium‐disilicate occlusal veneers (IPS e.max Press, Ivoclar). Restorations were adhesively cemented (Syntac Classic/Variolink II, Ivoclar) and exposed to thermomechanical fatigue (1.2 million cycles, 1.6 Hz, 49 N/ 5–55°C). Single load to failure was performed using a universal testing‐machine. A linear‐regression model was applied, pairwise comparisons used the Student–Newman–Keuls method (p < 0.05).Results: Three dentin‐based occlusal veneers (one DE‐1.0, two DE‐0.5) revealed cracks after fatigue exposure, which corresponds to an overall‐survival rate of 95%. Load to failure resulted in the following ranking: 2142 N(DE‐0.5) > 2105 N(E‐1.0) > 2075 N(E‐0.5) > 1440 N(DE‐1.5) > 1430 N(DE‐1.0). Thin (E‐1.0) and ultrathin enamel‐based occlusal veneers (E‐0.5) revealed high failure loads and surpassed the standard thickness dentin‐based veneers (DE‐1.5) significantly (p = 0.044, p = 0.022).Conclusion: All tested monolithic lithium disilicate occlusal veneers obtained failure loads above physiological chewing forces. Thin and ultrathin enamel‐based occlusal veneers outperformed the standard thick dentin‐based occlusal veneers.Clinical Significance: Minimally invasive enamel‐based occlusal veneer restorations with non‐retentive preparation design may serve as a conservative treatment option.