Objective: To analyze the clinical outcomes of all‐ceramic single crowns (SCs) and fixed dental prostheses (FDPs) supported by ceramic implants.Materials and Methods: Based on a focused question and customized PICO framework, electronic (Medline/EMBASE/Cochrane) and manual searches for studies reporting the clinical outcomes of all‐ceramic SCs and FDPs supported by ceramic implants ≥12 months were performed. The primary outcomes were reconstruction survival and the chipping proportion. The secondary outcomes were implant survival, technical complications, and patient‐related outcome measurements. Meta‐analyses were performed after 1, 2, and 5 years using random‐effect meta‐analyses.Results: Eight of the 1,403 initially screened titles and 55 full texts were included. Five reported on monolithic lithium disilicate (LS2) SCs, one on veneered zirconia SCs, and two on veneered zirconia SCs and FDPs, which reported all on cement‐retained reconstructions (mean observation: 12.0–61.0 months). Meta‐analyses estimated a 5‐year survival rate of 94% (95% confidence interval [CI]: 82%–100%) for overall implant survival. Reconstruction survival proportions after 5 years were: monolithic LS2, 100% (95%CI: 95%–100%); veneered zirconia SCs, 89% (95%CI: 62%–100%); and veneered zirconia FDPs 94% (95%CI: 81%–100%). The chipping proportion after 5 years was: monolithic LS2, 2% (95%CI: 0%–11%); veneered zirconia SCs, 38% (95%CI: 24%–54%); and veneered zirconia FDPs, 57% (95%CI: 38%–76%). Further outcomes were summarized descriptively.Conclusions: Due to the limited data available, only tendencies could be identified. All‐ceramic reconstructions supported by ceramic implants demonstrated promising survival rates after mid‐term observation. However, high chipping proportions of veneered zirconia SCs and, particularly, FDPs diminished the overall outcome. Monolithic LS2 demonstrated fewer clinical complications. Monolithic reconstructions could be a valid treatment option for ceramic implants.
10 November 2024 in Journal of Esthetic and Restorative Dentistry
Objectives: To analyze survival and complication rates for anterior and premolar laminate‐veneers out of different ceramic materials (feldspathic, leucite‐reinforced glass–ceramic [LRGC], lithium‐disilicate [LDS] and zirconia).Material and Methods: A systematic literature search was conducted across multiple databases for clinical studies on ceramic laminate‐veneers with a minimum‐follow‐up of ≥ 1 year. The date of last search was on February 19, 2024. Survival, technical, esthetic and biological events were assessed for different laminate‐veneer materials at three observation periods (short‐ [1–3 years], mid‐ [4–6 years] and long‐term [≥ 7 years]).Results: Twenty‐nine studies were included. Meta‐analysis revealed a pooled survival‐rate of 96.13% for feldspathic, 93.70% for LRGC and 96.81% for LDS at 10.4 years. No difference was found between materials. Complication rates (technical/esthetic/biological) were as follows: Feldspathic: 41.48%/19.64%/6.51%; LRGC: 29.87%/17.89%/4.4%; LDS: 6.1%/1.9%/0.45% at 10.4 years. Zirconia showed a 100% survival‐rate with no complications at 2.6 years. No long‐term data was available for zirconia.Conclusions: Feldspathic, LRGC and LDS laminate‐veneers showed high survival‐rates at long‐term observation. LDS slightly outperforms feldspathic and LRGC laminate‐veneers with lower long‐term complication rates. More studies providing long‐term data on zirconia laminate‐veneers are needed.Clinical Significance: Ceramic laminate‐veneers are a reliable treatment option. LDS may be preferred as a restorative material for long‐term success.
The demands for dental materials continue to grow, driven by the desire to reach a better performance than currently achieved by the available materials. In the dental restorative ceramic field, the structures evolved from the metal-ceramic systems to highly translucent multilayered zirconia, aiming not only for tailored mechanical properties but also for the aesthetics to mimic natural teeth. Ceramics are widely used in prosthetic dentistry due to their attractive clinical properties, including high strength, biocompatibility, chemical stability, and a good combination of optical properties. Metal-ceramics type has always been the golden standard of dental reconstruction. However, this system lacks aesthetic aspects. For this reason, efforts are made to develop materials that met both the mechanical features necessary for the safe performance of the restoration as well as the aesthetic aspects, aiming for a beautiful smile. In this field, glass and high-strength core ceramics have been highly investigated for applications in dental restoration due to their excellent combination of mechanical properties and translucency. However, since these are recent materials when compared with the metal-ceramic system, many studies are still required to guarantee the quality and longevity of these systems. Therefore, a background on available dental materials properties is a starting point to provoke a discussion on the development of potential alternatives to rehabilitate lost hard and soft tissue structures with ceramic-based tooth and implant-supported reconstructions. This review aims to bring the most recent materials research of the two major categories of ceramic restorations: ceramic-metal system and all-ceramic restorations. The practical aspects are herein presented regarding the evolution and development of materials, technologies applications, strength, color, and aesthetics. A trend was observed to use high-strength core ceramics type due to their ability to be manufactured by CAD/CAM technology. In addition, the impacts of COVID-19 on the market of dental restorative ceramics are presented.
6 January 2022 in Journal of Esthetic and Restorative Dentistry
Objective: To evaluate the effect of ceramic thicknesses, bonding surface (enamel vs. dentin), and preparation design (box vs. no box) on the fatigue survival and failure load of minimally invasive full‐veneer restorations.Materials and Methods: Human‐premolars (n = 60) were divided into five test groups (n = 12). All teeth received full‐veneer preparation with the following occlusal/labial thicknesses: standard: 1.5/0.8 mm; thin: 1.0/0.6 mm; ultrathin 0.5/0.4 mm. Preparations for each ceramic thickness were refined in enamel (E‐1.0 and E‐0.5) or dentin (D‐1.5, D‐1.0, and D‐0.5). Control groups DB‐1.5, EB‐1.0, and EB‐0.5 received box preparations. Monolithic lithium disilicate restorations (IPS‐e.max‐Press, Ivoclar Vivadent) were adhesively cemented (Syntac‐Classic/Variolink‐II, Ivoclar Vivadent) and subjected to cyclic mechanical loading (F = 49 N, 1.2 million cycles) with simultaneous thermocycling (5–55°C). All specimens were exposed to single load‐to‐failure. Pair‐wise differences were calculated by using a linear regression model and Student–Newman–Keuls method (p < 0.05).Results: All full‐veneers of group D‐1.5, E‐1.0, E‐0.5, DB‐1.5, EB‐1.0, and EB‐0.5 survived fatigue. Two full‐veneers (D‐1.0 and D‐0.5) revealed cracks during fatigue, resulting in an overall fatigue survival rate of 98.1%. Mean load‐to‐failure values (N) were as followed: 1005 (D‐1.5); 866 (D‐1.0); 816 (D‐0.5); 1495 (E‐1.0); 1279 (E‐0.5); 1129 (DB‐1.5); 1087 (EB‐1.0); and 833 (EB‐0.5). Irrespective of ceramic thicknesses, enamel‐based full‐veneers resulted in higher failure loads than dentin‐based restorations. Box preparation reduced the failure loads of thin and ultrathin enamel‐based restorations.Conclusion: All tested monolithic lithium disilicate full‐veneer restorations exceeded physiological masticatory forces. Minimally invasive full‐veneer restorations with enamel as a bonding surface and a non‐retentive preparation design showed superior performance.Clinical Significance: Enamel‐based non‐retentive full‐veneers made of monolithic lithium disilicate may serve as a reliable and esthetical minimally invasive treatment option for premolars.
1 January 2021 in The Journal of Advanced Prosthodontics
Objective: To analyze the influence of restoration design (partial‐coverage restoration vs. crown) and ceramic layer thickness on the performance and failure loads of CAD/CAM‐fabricated lithium disilicate (LDS) reconstructions on molars after fatigue.Materials and Methods: Seventy‐two posterior monolithic CAD/CAM‐fabricated LDS restorations (IPS e.max CAD, Ivoclar Vivadent) with different occlusal/buccal ceramic layer thicknesses (1.5/0.8, 1.0/0.6, and 0.5/0.4 mm) and restoration designs (PCR: non‐retentive full‐veneer/partial‐coverage restoration, C: crown,) were investigated and divided into six groups (n = 12, test: PCR‐1.5, PCR‐1.0, PCR‐0.5; control: C‐1.5, C‐1.0, C‐0.5). LDS restorations were adhesively bonded (Variolink Esthetic DC, Ivoclar Vivadent) to dentin‐analogue composite dies (Z100, 3M ESPE). All specimens were subjected to thermomechanical loading (1.2 million cycles, 49 N, 1.6 Hz, 5–55°C) and exposed to single load to failure testing. Failure analysis was performed with light and scanning electron microscopies. Data were statistically analyzed using ANOVA, Tukey‐Test, and t‐test (p < 0.05).Results: Eight crown samples (C‐0.5) and one PCR specimen (PCR‐0.5) revealed cracks after fatigue, resulting in an overall success rate of 87.5% (crowns: 75%, PCRs: 96.88%). Direct comparisons of PCRs versus crowns for thicknesses of 0.5 mm (p < 0.001) and 1.0 mm (p = 0.004) were significant and in favor of PCRs. Minimally invasive PCRs (0.5 and 1.0 mm) outperformed crowns with the identical ceramic thickness. No difference was detected (p = 0.276) between thickness 1.5 mm PCRs and crowns.Conclusions: Minimally invasive monolithic CAD/CAM‐fabricated posterior LDS PCRs (0.5 and 1.0 mm) resulted in superior failure load values compared to minimally invasive crowns. Minimally invasive crowns (0.5 mm) are prone to cracks after fatigue.Clinical Significance: Minimally invasive CAD/CAM‐fabricated LDS PCR restorations with a non‐retentive preparation design should be considered over single crowns for molar rehabilitation.