The pitting corrosion resistance of AISI 1045 carbon steel with as-quenched, tempered, and low-carbon martensitic microstructures was investigated in boric-borate buffer solutions with and without NaCl. Analysis by micro-scale polarization found that tempering and decarburizing treatments decreased the pitting corrosion resistance of as-quenched martensite. The high corrosion resistance of the as-quenched martensite was likely due to the large amount of interstitial carbon. The pitting corrosion resistances of as-quenched martensite, primary ferrite, and pearlite were compared using micro-scale polarization measurements. It was determined that the pitting corrosion resistances of the typical steel structures were ordered as follows: (high) as-quenched martensite > tempered martensite ≈ primary ferrite > pearlite (low). The pitting corrosion resistance of steel was shown to depend on its microstructure.
The initiation site and morphology during the early stage of pitting on AISI 1045 carbon steel that has a microstructure of primary ferrite and pearlite were investigated in boric-borate buffer solutions with and without NaCl at pH 8.0. The pits initiated by micro-scale polarization were in the pearlite only and not in primary ferrite. In situ real-time observations during the micro-scale polarization of pearlite in a boric-borate buffer solution with 100 mM NaCl indicated that the pits were polygonal or rod-like in shape. In addition, it was found that the pit growth direction was the same as that of the pearlite lamellae that consisted of ferrite and cementite. Field-emission electron probe micro analysis detected segregated points of sulfur in the ferrite lamellae. On the basis of their etching behavior in 3% nital, the corrosion resistance of the cementite was estimated to be higher than that of the ferrite lamellar structure. Thus, pits readily initiated in the ferrite lamellae and proceeded along the ferrite lamellae.
2 August 2019 in Journal of the Electrochemical Society