The paper presents research program of bond between glass fiber reinforced polymer bars and concrete in reference to the steel bars. Bond between the reinforcement and concrete is a crucial parameter governing a behaviour of reinforced concrete members and transferring of the internal forces from concrete to the reinforcement. The use of FRP bars as an equivalent reinforcement to steel in concrete structures has increased in recent years. The FRP bars are very different from steel, mainly due to much lower elasticity modulus and their anisotropic structure. Good performance of FRP reinforced concrete requires sufficient interfacial bond between bars and concrete. However, there are no specific standards referring to the surface preparation of these bars, that leads to variable bond behaviour of the composite reinforcement to the concrete. The objective of the study was to investigate the influence of variable parameters on the bond behaviour to concrete. The experimental program consisted of eighteen beam bond specimens varying in: bar diameter (12mm, 16mm, 18mm) and type of reinforcement (GFRP sand – coated and steel bars). Although the GFRP bars indicated good bond behaviour to concrete, the average bond strength was slightly lower than that of steel reinforcement of 16mm and 18 mm, while it was higher for the GFRP bars of 12mm diameter.
This paper aims to investigate the shear failure mechanisms in beams reinforced with longitudinal and transverse glass fibre reinforced polymer bars. It is a part of comprehensive research on shear in concrete beams reinforced with steel and GFRP bars. The experimental program is composed of six real-scale single-span, simply-supported T-cross section concrete beams. The beams varied mainly with respect to the longitudinal reinforcement ratio (2.91% and 3.69%), bar diameter (25mm and 28mm, respectively) and transverse reinforcement ratio (0.16% and 0,33%). The paper presents test results, cracking patterns, failure modes and an analysis of the influence of variable parameters on the shear behaviour of elements.
The paper presents results of experimental tests carried out on concrete beams reinforced with glass fibre polymer reinforced (GFRP) bars, which have become recently one of the main substitutes for traditional steel reinforcement. GFRP bars were used in this research as the longitudinal and transverse reinforcement. An objective of the study was to investigate the influence of the shear reinforcement ratio on the shear capacity of GFRP reinforced concrete beams in comparison with the corresponding beam without shear reinforcement. Single-span, simply-supported T-section beams reinforced in flexure with 5 GFRP bars of 25 mm diameter were reinforced in shear with closed GFRP stirrups of 8 mm diameter applied in three variable spacings: 250 mm, 200 mm and 120 mm. The analysis of test results, failure modes and shear capacity is discussed in the paper in respect to investigated parameters.
The paper presents test results of reinforced concrete beams flexurally strengthened with Carbon Fibre Reinforced Polymer (CFRP) laminates using the Near Surface Mounted (NSM) technique. RC beams with a cross section of 200 x 400 mm were tested in four-point bending. Two RC beams were strengthened with one NSM CFRP laminate installed into the concrete cover on the bottom side of the beam. One of the beams was strengthened under the self-weight (B10.1) and the second one under initial preloading equal to 83% of the ultimate load of the reference beam (B10.1o). Failure mechanisms, cracking pattern and flexural behaviour of the beams are described in the paper. All the strengthened beams failed by rupture of the CFRP laminates followed by the internal steel reinforcement yielding. High strengthening efficiency of the NSM strengthening was confirmed by 109% and 130% when compared with the non-strengthened beam, respectively for beams B10.1 and B10.1o.