The effects of solution treatment and annealing temperature on the microstructure and mechanical properties of a new TWIP steel that was alloyed from aluminum (Al), silicon (Si), vanadium (V), and molybdenum (Mo) elements were investigated by a variety of techniques such as microstructural characterization and room tensile testing. The austenite grain size grew slowly with the increase in annealing temperature. The relatively weak effect of the solution treatment and annealing temperature on the austenite grain size was attributed to the precipitation of MC and M2C, which hindered the growth of the austenite grain. The plasticity of the TWIP steel in cold rolling and annealing after solution treatment was obviously higher than that in cold rolling and annealing without solution treatment. This was because the large-size precipitates redissolved in the matrix after solution treatment, which were not retained in the subsequently annealed structure. Through cold rolling and annealing at 800 °C after solution treatment, the prepared steel exhibited excellent strength and plasticity simultaneously, with a yield strength of 877 MPa, a tensile strength of 1457 MPa, and an elongation of 46.1%. The strength improvement of the designed TWIP steel was mainly attributed to the grain refinement and precipitation strengthening.
Grain refinement is a satisfying method to enhance the comprehensive performance of Mg alloys, and using grain refiners to improve the quality of Mg castings has become a common practice in the current casting industry. In this study, the effects of Al-CeO2-Mg grain refiner addition on microstructure, cast fluidity, and mechanical properties of AZ91 alloy were systemically investigated by OM, SEM, DSC, TEM, sand Archimedean spiral mold fluidity test, and tensile test. The results show that the Al-CeO2-Mg grain refiner has a remarkable effect on as-cast AZ91 alloy including notable grain refinement, enhancement of cast fluidity, and improvement of tensile properties. The average grain size of AZ91 alloy is refined by 63% with 1.0wt.% Al-CeO2-Mg grain refiner. Meanwhile, the casting flow length of the as-cast AZ91 alloy is increased from 332 mm to 440 mm. The improvement of cast fluidity is attributed to the decreased liquidus temperature, shortening of solid-liquid two-phase temperature range, and refinement of microstructure.
Based on the idea of integrated computational materials Engineering (ICME), this research applies a digital integrated computing platform integrating ProCAST and MATLAB software. The effects of Fe and Zn contents on the microstructure and properties of die-casting Al–10Si–Mg alloy was investigated through numerical simulation and experimental characterization. The results show that with Fe and Zn contents of 1.30 and 0.25 wt.%, respectively, the grain size and porosity of the die-cast parts are the smallest, and the yield strength and tensile strength are 203 MPa and 313 MPa, respectively. Compared with the addition of 0.14 wt.% Fe and 0.01 wt.% Zn, the increase was 16% and 15.5%, respectively. When the Fe content is higher than 1.30 wt.%, the size of the β-Al5FeSi phase in the alloy matrix increases. Moreover, as the Fe content increases, the morphology of the β-Al5FeSi transforms from elongated to a needle-like shape, which increases brittleness and reduces elongation, tensile strength, and yield strength. When 0.25 wt.% Zn is added, the segregation phenomenon of eutectic Si in the Al–10Si–Mg alloy is inhibited and the tensile strength and yield strength are improved. However, with the increase in Zn content to 0.95 wt.%, there is the coarsening of eutectic Si, resulting in a decreased elongation and decreased mechanical properties. The optimization method of the integrated computing platform greatly simplifies the computing cycle and improves work efficiency.
Grain refinement is a crucial technological strategy for achieving microstructural homogenization and enhancing the mechanical performance of aluminum alloys. This study examines the synergistic effects of trace additions of NbB2 and Ti on microstructural refinement and the enhancement of mechanical properties in high-pressure die-cast (HPDC) Al-Si series alloys. Through systematic investigations utilizing scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM) analyses, the mechanisms by which trace additions of NbB2 and Ti contribute to the synergistic refinement and strengthening of mechanical properties in HPDC Al-Si alloys are elucidated. The incorporation of NbB2 effectively refines both the externally solidified crystals (ESCs) and secondary α-AlII grains. The combined addition of NbB2 and Ti further amplifies this effect, resulting in optimal refinement outcomes in the Al-Si series alloy, characterized by an ESC grain size of 19.1 μm and an area fraction of 27.5%, as well as an α-AlII grain size of 6 μm. TEM observations reveal the formation of a Ti-rich transition layer between NbB2 and Al with the synergistic addition of Ti and NbB2, which fills interface nucleation vacancies and enhances refinement performance.
Grain refinement represents a critical approach in optimizing the as-cast microstructure of magnesium alloys, playing a pivotal role in the development of high-performance magnesium alloys. In the present research, a novel Al-Ce-C-O-Mg grain refiner was fabricated using an innovative rolling-assisted process, and the influence of the grain refiner on the grain size evolution of as-cast AZ91 alloy was systematically examined. The Al-Ce-C-O-Mg grain refiner prepared by the rolling-assisted process contains two types of effective refining particles—MgAl2O4 and Al4C3. These particles can act as potent nucleation sites for α-Mg in the melt, promoting efficient nucleation and achieving significant grain refinement. By adding 1.0 wt.% of the Al-Ce-C-O-Mg grain refiner to the AZ91 alloy, the grain size of the original AZ91 alloy was reduced by 73%. Moreover, adding a refiner facilitated the transformation of the coarse β-Mg17Al12 phase morphologies into a more uniformly distributed and dispersed form. The addition of 1.0 wt.% Al-Ce-C-O-Mg grain refiner to the AZ91 alloy resulted in significant improvements in its mechanical properties. The ultimate tensile strength (UTS), yield strength (YS), and elongation (EL) increased from 158 MPa, 104 MPa, and 3.9% to 203 MPa, 121 MPa, and 6.3%, respectively. The grain refiner developed in this study demonstrates promising potential for application in Mg alloys.