The (Ba0.85Ca0.15) (Ti0.90Zr0.10)O3 + x Y3+ + x Nb5+ (abbreviated as BCZT-x(Nb + Y), x = 0 mol%, 0.05 mol%, 0.1 mol%, 0.2 mol%, 0.3 mol%) lead-free piezoceramics samples were prepared by a traditional solid-state sintering method. And the effects of Yttrium and Niobium elements (Y3+ and Nb5+) co-doping on the defect, phase and structure, microstructure, and comprehensive electrical properties have been investigated. Research results show that the Y and Nb elements co-doping can dramatically enhance piezoelectric properties. It is worth noting that XPS defect chemistry analysis, XRD phase analysis and TEM results together show that a new phase of double perovskite structure Barium Yttrium Niobium Oxide (Ba2YNbO6) is formed in the ceramic, and the XRD Rietveld refinement and TEM results show the coexistence of the R-O-T phase. Both these two reasons together lead to significant performance improvements of piezoelectric constant (d33) and planar electro-mechanical coupling coefficient (kp). The functional relation between temperature and dielectric constant testing results present that the Curie temperature increases slightly, which shows the same law as the change of piezoelectric properties. The ceramic sample reaches an optimal performance at x = 0.1% of BCZT-x(Nb + Y), where d33 = 667 pC/N, kp = 0.58, εr = 5656, tanδ = 0.022, Pr = 12.8 μC/cm2, EC = 2.17 kV/cm, TC =92 °C, respectively. Therefore, they can be used as potential alternative materials to lead based piezoelectric ceramics.
To synergistically integrate piezoelectric and varistor functionalities in a single material, PNN-PZT piezoelectric powder (abbreviated as P) and ZnO-based varistor powder (abbreviated as Z) were utilized to fabricate PZT-ZnO composite ceramics (denoted as PZm) via conventional solid-state sintering. The P/Z molar ratio was regulated to 1/0.9, 1/1.05, 1/1.2, 1/1.35, and 1/1.5 to systematically study its influence on the phase composition, microstructure, and electrical properties of the composites. XRD, SEM, EDS characterization, and electrical performance tests were carried out. Results indicate that all PZm samples exhibit the biphasic coexistence of perovskite (piezoelectric phase) and wurtzite (varistor phase) without impurity phases, consisting of large perovskite grains with distinct edges and small wurtzite grains with smooth surfaces. The PZ3 sample (P/Z = 1/1.2) achieves optimal comprehensive properties: d33 = 161 pC/N, kp = 0.25, Ɛr = 2527, tan δ = 3.83%, E1mA = 1396 V/mm, IL = 8.2 mA, α = 22.06. This work confirms the synergistic optimization of piezoelectric and varistor properties in PZT-ZnO composites, providing a reliable experimental basis for the formulation design and performance regulation of multifunctional ceramics.