Laser powder bed fusion (LPBF) is an additive manufacturing process that has gained interest for its material fabrication due to multiple advantages, such as the ability to print parts with small feature sizes, good mechanical properties, reduced material waste, etc. However, variations in the key process parameters in LPBF may result in the instantiation of porosity defects and variation in build rate. Particularly, volumetric energy density (VED) is a variable that encapsulates a number of those parameters and represents the amount of energy input from the laser source to the feedstock. VED has been traditionally used to inform the quality of the printed part but different values of VED are presented as optimal values for certain material systems. An optimal VED value can be maintained by changing the key process parameters so that various combinations yield a constant value. In this study, an optimal constant VED value is maintained while printing SS316L with variable key processing parameters. Porosity analysis is performed using optical microscopy, as well as X-ray computed tomography, to reveal the volume density and distribution of those pores. Two primary defect categories are identified, namely lack of fusion and porosity induced by balling defects. The findings indicate that, even at optimal VED, variations in process parameters can significantly influence defect type, underscoring the sensitivity of defect formation to the variation of these parameters. Furthermore, a minor change in the build rate, driven by adjustments in process parameters, was found to influence defect categories. These findings emphasize that fine tuning the process parameters and build rate is essential to minimize defects. Finally, fiducial marks have been identified as a source of unintentional porosity defects. These results enable the refinement of process parameters, ultimately optimizing LPBF to achieve enhanced material density and expedite the printing.
Electric Field Assisted Sintering (EFAS, also referred to as spark plasma sintering) is a powerful technology for the consolidation of powder materials. The high heating rate during the sintering process is critical for minimizing energy consumption, but it can also cause microstructure heterogeneities in sintered parts, such as spatially varied porosity. The examination of localized porosity usually requires the use of a scanning electron microscope with a carefully prepared surface. In this paper, photothermal radiometry is used to measure local thermal diffusivity and extract localized porosity of EFAS-sintered parts by using a percolation-threshold model. Applying this approach, we identified the radial position-dependent porosity variation in EFAS parts, which is likely formed due to the large temperature gradient during the sintering process. This approach has a unique advantage because it can measure samples with minimal or no surface preparation, enabling the possibility of in situ characterization in EFAS with proper system modification. Necessary modifications on the measurement approach for EFAS deployment and in situ characterization are also discussed.