Since steel cleanness comes to the fore of steel producers worldwide, it is necessary to understand the formation mechanism and modification of non-metallic inclusions (NMIs) in more detail. One central point is the identification of the source of especially interfering NMIs to prevent their evolution in the future. The present study applies two approaches to determine the source of NMIs in Ti-stabilized ultra-low carbon (ULC) steels—the active and the passive tracing. Both approaches are applied to an industrial experiment. The active tracing technique is focused on investigating the clogging layer formation in submerged entry nozzles and, hence, the origin of alumina particles. This method adds rare earth elements (REEs) directly to the melt to mark pre-existing deoxidation products at a certain point of the steelmaking process. The main concern of the passive method, the so-called REE fingerprint, is the determination of the source of mesoscopic NMIs. For the REE fingerprint, the pre-existing concentration of REEs in different potential sources and the investigated NMIs are measured by using an inductively coupled plasma mass spectrometer (ICP-MS). The resulting patterns are compared after normalizing the contents to chondrites, and the NMIs’ origins are identified. Concerning the EDS analysis and the resulting patterns from the REE fingerprint, the mold slag and, respectively, the casting powder were the sources of the investigated NMIs.
Non-metallic inclusions (NMIs) in steel have a detrimental effect on the processing, mechanical properties, and corrosion resistance of the finished product. This is particularly evident in the case of macroscopic inclusions (>100 µm), which are rarely observed in steel castings produced using state-of-the-art technologies, whereby casting parameters are optimized towards steel cleanliness, and post-treatment steps such as vacuum arc remelting (VAR) are used, but frequently result in the rejection of the affected product. To improve production processes and develop effective countermeasures, it is essential to gain a deeper understanding of the origin and formation of NMIs. In this study, the potential of elemental and isotopic fingerprinting to trace the sources of macroscopic oxide NMIs found in VAR-treated steel ingots using SEM-EDX, inductively coupled plasma mass spectrometry (ICP-MS), laser ablation ICP-MS (LA-ICP-MS), and laser ablation multicollector ICP-MS (LA-MC-ICP-MS) were exploited. Following this approach, main and trace element content and 87Sr/86Sr isotope ratios were determined in two specimens of macroscopic NMIs, as well as in samples of potential source materials. The combination of the data allowed the drawing of conclusions about the processes leading to the formation of these inclusions. For both specimens, very similar results were obtained, indicating a common mechanism of formation. The inclusions were likely exogenous in origin and were primarily composed of calcium–aluminum oxides. They appeared to have undergone chemical modification during the casting and remelting process. The results indicate that particles from the refractory lining of the casting system most likely formed the macroscopic inclusions, possibly in conjunction with a second, calcium-rich material.