Kathrin Thiele

Ms. Kathrin Thiele

Chair of Ferrous Metallurgy, Montanuniversität Leoben, Leoben, Steiermark, Austria
orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
4 October 2022 in Ironmaking & Steelmaking: Processes, Products and Applications
Verified
Journal Article
Open access
Kathrin ThieleKathrin Thiele
Kathrin Thiele
PPPeter Presoly
Peter Presoly
Daniel ErnstDaniel Ernst
Daniel Ernst
SBShashank Ramesh Babu
Shashank Ramesh Babu
Susanne MichelicSusanne Michelic
Susanne Michelic
Different alloying concepts to trace deoxidation products, mainly aluminium oxides, using rare earth elements (REEs), were tested on the laboratory scale by melting trials with a high-frequency remelting furnace. Lanthanum and Cerium, which belong to the group of light REEs, were used for these experiments. The formed multiphase inclusions were characterized by scanning electron microscopy with energy dispersive spectroscopy. Concerning the higher atomic numbers of REEs, traced non-metallic inclusions (NMIs) seem brighter than the steel matrix compared to deoxidation products. REE-traced aluminium oxides showed a primarily heterogeneous and almost globular morphology. The mean equivalent circle diameter of REE-containing NMIs is for all trials similar and is about 2 µm. The experimental results pointed out that the recovery rates of the various alloying concepts differ only slightly. In contrast, the values mainly depend on the surface-to-volume ratio and the amount of oxygen in the melt. GRAPHICAL ABSTRACT

15 January 2024 in Metals
Verified
Journal Article
Open access
PDF file
Kathrin ThieleKathrin Thiele
Kathrin Thiele
CTChristoph Truschner
Christoph Truschner
CWChristoph Walkner
Christoph Walkner
TMThomas C Meisel
Thomas C Meisel
SISergiu Ilie
Sergiu Ilie
Susanne MichelicSusanne Michelic
Susanne Michelic
Since steel cleanness comes to the fore of steel producers worldwide, it is necessary to understand the formation mechanism and modification of non-metallic inclusions (NMIs) in more detail. One central point is the identification of the source of especially interfering NMIs to prevent their evolution in the future. The present study applies two approaches to determine the source of NMIs in Ti-stabilized ultra-low carbon (ULC) steels—the active and the passive tracing. Both approaches are applied to an industrial experiment. The active tracing technique is focused on investigating the clogging layer formation in submerged entry nozzles and, hence, the origin of alumina particles. This method adds rare earth elements (REEs) directly to the melt to mark pre-existing deoxidation products at a certain point of the steelmaking process. The main concern of the passive method, the so-called REE fingerprint, is the determination of the source of mesoscopic NMIs. For the REE fingerprint, the pre-existing concentration of REEs in different potential sources and the investigated NMIs are measured by using an inductively coupled plasma mass spectrometer (ICP-MS). The resulting patterns are compared after normalizing the contents to chondrites, and the NMIs’ origins are identified. Concerning the EDS analysis and the resulting patterns from the REE fingerprint, the mold slag and, respectively, the casting powder were the sources of the investigated NMIs.

26 February 2023 in Advanced Engineering Materials
Verified
Journal Article
Open access
Kathrin ThieleKathrin Thiele
Kathrin Thiele
RMRobert Musi
Robert Musi
SBShashank Ramesh Babu
Shashank Ramesh Babu
Susanne MichelicSusanne Michelic
Susanne Michelic
Tracing by means of the light rare earths (REs), particularly La and Ce, is a state‐of‐the‐art method used to track deoxidation products during the steelmaking process. Traced heterogeneous multiphase inclusions are analyzed using scanning electron microscopy with energy‐dispersive spectroscopy (SEM/EDS) to perform a 2D characterization. The sequential chemical extraction technique is implemented for a 3D investigation to determine traced particles’ actual sizes and shapes. The automated SEM/EDS measurement must be optimized since RE oxides appear brighter in the backscattered electron images due to their high atomic numbers. Therefore, two grayscales are implemented for the detection of RE‐containing multiphase inclusions. Within this technique, individual RE‐traced heterogeneous nonmetallic inclusions (NMIs) are counted as separate particles. Thus, the measured NMIs must be recombined, which is achieved using a self‐developed MATLAB tool. The extracted particles are also analyzed by automated and manual SEM/EDS measurements to determine the 3D morphologies and sizes of traced NMIs.

31 December 2023 in Steel Research International
Verified
Journal Article
Open access
CTChristoph Truschner
Christoph Truschner
Kathrin ThieleKathrin Thiele
Kathrin Thiele
SISergiu Ilie
Sergiu Ilie
RRRoman Rössler
Roman Rössler
AJAlfred Jungreithmeier
Alfred Jungreithmeier
Susanne MichelicSusanne Michelic
Susanne Michelic
The continuous casting of Al-killed Ti-stabilized interstitial free steels is often affected by clogging. By today, the mechanism behind this phenomenon is not entirely clarified. The active tracing method, which involves the direct addition of rare-earth elements (REEs), enables tracking of nonmetallic inclusions (NMIs) over process time. Due to the high oxygen affinity of these elements, preexisting NMIs are partially reduced and marked by this tracer. Using scanning electron microscopy with energy-dispersive spectroscopy, it is possible to differentiate such labeled NMIs from particles formed at later stages in the process by the absence of these tracing elements. Active tracing is used in industrial and laboratory settings to trace preexisting alumina NMIs with La or Ce. In the investigation, it is revealed that the number of small NMIs increases after the addition of REEs, and subsequently, the size increases again after FeTi is alloyed. In both settings, traced and untraced Al–Ti oxides are found. The separation tendency of traced NMIs is studied over time by analyzing the composition of the slags. Furthermore, the impact of deoxidation products on the formation of the clogging layer within the submerged entry nozzle is investigated, indicating that these NMIs contribute to its formation.

20 December 2023 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
Kathrin ThieleKathrin Thiele
Kathrin Thiele
RMRobert Musi
Robert Musi
TPThomas Prohaska
Thomas Prohaska
JIJohanna Irrgeher
Johanna Irrgeher
Susanne MichelicSusanne Michelic
Susanne Michelic

6 February 2024 in BHM Berg- und Hüttenmännische Monatshefte
Verified
Journal Article
Open access
PDF file
MSM. Schickbichler
M. Schickbichler
Kathrin ThieleKathrin Thiele
Kathrin Thiele
Susanne MichelicSusanne Michelic
Susanne Michelic
Zusammenfassung: In metallurgischen Anwendungen nimmt der Einsatz von Seltenen Erden (SE) eine zunehmend größere Rolle ein. Diese werden in modernen Herstellungsprozessen nicht nur als Kornfeinungsmittel eingesetzt, sondern auch zur Markierung von Desoxidationsprodukten. Durch das Tracen der Einschlüsse (NME) ist es möglich, die Modifikation von beispielsweise Aluminiumoxiden über den Prozess zu verfolgen und zu erforschen. Aufgrund der teilweisen Reduktion der bestehenden NME kommt es zur Veränderung dieser hinsichtlich der chemischen und physikalischen Eigenschaften, sowie ihrer Morphologie.Die Modifikation der Einschlüsse mittels SE kann ebenfalls ihre Löslichkeit in verschiedenen Chemikalien beeinflussen. Daher liegt ein Fokus der durchgeführten Studie darauf, die Stabilität der gebildeten komplexen mehrphasigen SE-Al-Oxide mithilfe häufig angewandter Extraktionsmethoden zu untersuchen.Dabei kommt es zur Evaluierung der Anwendbarkeit von elektrolytischer und sequenzieller chemischer Extraktionstechnik für SE-haltige Einschlüsse. Bei den Proben für diese Studie handelt es sich um Ultra-Low Carbon (ULC)-Stähle, die durch Ce modifizierte Aluminiumoxide beinhalten. Ziel ist es, zusätzlich zur Überprüfung der Stabilität dieser mehrphasigen Einschlüsse bei verschiedenen Extraktionsmethoden auch die Anzahl an Einschlüssen pro Volumen zu prognostizieren. Dazu findet eine Berechnung der NME-Konzentration mittels des Modells nach Woodhead statt und anschließend werden die Ergebnisse dieser Modellrechnung mit der gemessenen Anzahl an NME pro Volumen verglichen.